Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (3): 21-148    DOI:
Current Issue | Archive | Adv Search |
DEPENDENCE OF HYDROGEN CONTENT ON HYDRIDE STRUCTURE AND YIELD STRENGTH OF TITANIUM PLATE
by WANG Ruikun; WANG Deming (Beijing General Research Institute of Non-ferrous Metals)
Cite this article: 

by WANG Ruikun; WANG Deming (Beijing General Research Institute of Non-ferrous Metals). DEPENDENCE OF HYDROGEN CONTENT ON HYDRIDE STRUCTURE AND YIELD STRENGTH OF TITANIUM PLATE. Acta Metall Sin, 1986, 22(3): 21-148.

Download:  PDF(2870KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The yield strength of the pure Ti plate may be decreased at 540—650℃ for specimen containing H within the range of 60 to 80 ppm, but it is decreased no more in increasing H. The sharp upper-lower yield point is occurred on the stressstrain curve as H content less than 50 ppm at room temperature and 540℃, and disappeared as H over 50 ppm or at 650℃. Thus, the maximum interaction energy between H atom and dislocation in pure Ti was calculated to be 0.47—0.53 eV. The morphology of hydride in pure Ti was observed in the plate or needle shape. The hydride TiH_2 was found to be the structure of BCT or fcc as H content less or more than 80 ppm respectively. It is also observed under HVEM that the hydride in specimen containing 15 ppm H is of BCT structure.
Received:  18 March 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I3/21

1 #12.
2 #12.
3 Meyn, D.A., Hydrogen Damage, ASM, Metals Park, Ohio, 1977, p. 319.
4 Cottrell. A. H., 晶体的位错和范性流变,葛庭燧译,科学出版社,1960,p.148.
5 Heady, R.B., Corrosion, 9 (1978) , 303.
6 Hirsch, P.B.; Homwie, A.; Nickolson, R.B.; Pashley, D.W.; Whelan, M.J., Electron Microscopy of Thin Crystals, Butterworths, London, 1971, p. 325.T
No related articles found!
No Suggested Reading articles found!