Abstract  The low frequency internal friction of the cold-worked Ta wire with high purity was measured before and after hydrogen charging. It showed that a precipitation peak appears at higher temperature than that of H-SK peak, and at same time the latter is decreased in its height after charging. An additional twist shows remarkable influence on the precipitation peak. Aging at the temperature in which O atoms are able to migrate to the dislocations might completely eliminate the enhancement effect. The results indicate that the hydrides might preferentially precipitate on the dislocations. The precipitation peak is considered to be associated with the interaction between the dislocations and the hydrides.
Received:  18 March 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I3/26

1 Buck, O.; Thompson, D.O.; Wert, C.A., J. Phys. Chem. Solids, 32 (1971) , 2331.
2 Cannelli, G.; Cantelli, R., Appl. Phys., 3 (1974) , 325.
3 Chang, H.Y.; Wert, C.A., Acta Metall., 21 (1973) , 1233.
4 Yoshinari, O; Koiwa, M., Acta Metall., 30 (1982) , 1979.
5 Yoshinari, O; Koiwa, M., Acta Metall., 30 (1982) , 1987.
6 李广义;孙宗琦;曲开选等,第二届全国固体缺陷会议上宣读,1982.
7 Larche, F.C., Dislocations in Solids, Vol. 4, Ed. Nabarro, F.R. N, North-Holland, Amsterdam. 1979, p. 135.
8 Birnbaum, H.K.; Grossbeck, M.L.; Amano, M., J. Less-Common Met., 49 (1976) , 357.
9 Seeger, A.; Weller, W.; Diehl, J.; Pan, Zh,L.;Zhang. J. X.;Ke, T.S., Z. Metallk., 73 (1982) , 1.
10 Van Ooijen, D.J.; Van der Goot, A.S., Philips Res. Rep., 22 (1967) , 150.p
No related articles found!
No Suggested Reading articles found!