FRACTURE BEHAVIOUR OF FUSED QUARTZ PARTICULATE COMPOSITES
by WANG Runze; LIU Yanling (Luoyang Institute of Refractory Research)
Cite this article: 

by WANG Runze; LIU Yanling (Luoyang Institute of Refractory Research). FRACTURE BEHAVIOUR OF FUSED QUARTZ PARTICULATE COMPOSITES. Acta Metall Sin, 1986, 22(3): 117-123.

Download:  PDF(1024KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The fracture behaviour of the fused quartz particulate composites was investigated. It showed that the volume fraction of particles dispersed in the matrix leads to direct dependencies of the elastic modulus and fracture surface energy; inverse changes in bending strength as well as increasing in art exponential relation with work of fracture and thermal shock damage resistance parameter. The decohesion of the weak interface between particle and matrix may be considered as the origin of toughening.
Received:  18 March 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I3/117

1 Hasselman, D.P.H., J. Am. Ceram. Soc., 46 (1963) , 535.
2 Hasselman, D.P.H., J. Am. Ceram. Soc., 52 (1969) , 600.
3 Hasselman, D.P.H., J.Am Ceram. Soc., 49 (1966) , 68.
4 Lange, F.F., Philos. Mag., 22 (1970) , 983.
5 Green, D.J.; Nicholson, P.S.; Embury, J.D., J.Mater. Sci, 14 (1979) , 1413.
6 Khaund, A.K.; Nicholson, P.S., J.Mater. Sci., 15 (1980) , 177.
7 楼福珍;钮雁南;邹甫俊,耐火材料,(1980) ,№6,33.
8 Nakayama, J., J. Am. Ceram. Soc., 48 (1965) , 583.
9 Lange, F.F.. J.Am. Ceram. Soc., 54 (1971) , 614.
10 Uchno, J.J.; Bradt, R.C.; Hasselman, D.P.H., Am. Ceram. Soc, Bull., 55 (1976) , 665.
11 Nakayama, J.; Ishizuka, M., Am. Ceram. Soc. Bull, 45 (1966) , 666.5
No related articles found!
No Suggested Reading articles found!