| FACTORS IN WALL THICKNESS CHANGE OF SINKING TUBES |
| by YAO Ruohao; ZHONG Jianhua; LIU Xiaolin; MO Jianping (Jiangxi Institute of Metallorgy. Ganzhou) |
|
Cite this article:
by YAO Ruohao; ZHONG Jianhua; LIU Xiaolin; MO Jianping (Jiangxi Institute of Metallorgy. Ganzhou). FACTORS IN WALL THICKNESS CHANGE OF SINKING TUBES. Acta Metall Sin, 1986, 22(3): 124-131.
|
|
|
Abstract The ratio of tube diameter to wall thickness and the relative drawing stress were believed to be the factors in wall thickness change of sinking tubes. The critical coefficient, about 3.6—7.6, obtained in both consideration of mentioned factors together is wider than that, about 5—6, conventionally used in the production practice. The effect of the process conditions, such as: properties of material, reduction in each pass, total elongating passes, lubricating conditions, drawing speed, geometric parameters of die, etc. on the wall thickness change of sinking tubes has also been investigated theoretically and experimentally. It was shown that they attributes their functions to the variation of value of relative drawing stress from which the accurate caleulational formula and plot in estimation of wall thickness change are given for industrial production.
|
|
Received: 18 March 1986
|
1#12 2 #12 3 田中 浩,塑性加工,18(1977) ,901. 4 Slayer, R.A.C., Engineering Plasticity--Theory and Application to Metal Forming Processes, London, Macmillan, 1977, p. 294. 5 Johnson, W., Engineering Plasticity, Interscience, London and New York, 1973, p. 281. 6 周纪萍,铜加工,(1984) ,№1,65. 7#12 8 曹乃光,金属塑性加工原理,冶金工业出版社,1983,p.262. 9 #12 10 杨守山,有色金属塑性加工学,冶金工业出版社,1982,p.326 11 重有色金属材料加工手册编写组,重有色金属材料加工手册,(第4分册),冶金工业出版社,1980。p.159 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|