Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (5): 47-52    DOI:
Current Issue | Archive | Adv Search |
FORMATION OF Nb_3Sn DURING DIFFUSION USING A Sn-RICHED CuSn ALLOY
YANG Chuanzheng; HU Suhui (Shanghai Institute of Metallurgy; Academia Sinica)
Cite this article: 

YANG Chuanzheng; HU Suhui (Shanghai Institute of Metallurgy; Academia Sinica). FORMATION OF Nb_3Sn DURING DIFFUSION USING A Sn-RICHED CuSn ALLOY. Acta Metall Sin, 1986, 22(5): 47-52.

Download:  PDF(495KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Both empirical analysis and experimental investigation of the Nb-CuSn solidsolid diffusion couple arc shown that the Sn atoms in solid CuSn alloy diffuse into Nb lattice alone, but the diffusion of Nb atoms into CuSn alloy can be neglected. The only Nb_3Sn phase is formed with superior stability after diffusion. On the basis above mentioned, the discussion about the formation of Nb_3Sn during diffusion of solid-solid system was made. Furthermore, certain allied topics on that during solid-liquid diffusion were also interpreted briefly.
Received:  18 May 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I5/47

1 木村锡一;有贺美智雄,低温工学,14(1979) ,226. 木村锡一;渡辺牧夫,低温工学,15(1980) ,179.
2 Yamasaki, H.; Kimura, Y., Cryogenics, 22 (1982) , 89.
3 Suenga, M., Superconductor Materials Science, Metallurgy, Fabrication and Application, Eds. Foner, S.; Schwartz, B.B., Plenum Press, New York, 1981, p. 201.
4 Suenaga, M.; Sampson, W.B., Appl. Phys. Lett., 20 (1972) , 443.
5 官世明;赵惠玲,胡素辉,低温物理,7(1985) ,№ 3,199.
6 #12
7 Morowe, S., Deffects and Diffusion in Solid, an Introduction, Elsevier Scientific Publ., Amsterdam-Oxford, New York, 1980, p. 392.
8 Miedema, A.R., J. Less-Common Met., 32 (1973) , 117.
9 Raynor, G.V., J. Less-Common Met., 29 (1972) , 333.
10 Farrell, H.H.; Gilmer, G.H.; Suenaga, M., J. Appl. Phys., 45 (1974) , 4025.
11 Smather, D.B.; Larbalestier, D.C., Filamentary A-15 Superconductors, Eds. Suenaga, M; Clark, A. F., Plenum Press, New York, 1980, p. 143.
12 Suenaga, M.; Jansen, W., Appl. Phys. Lett., 43 (1983) , 791.H
No related articles found!
No Suggested Reading articles found!