Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (5): 106-111    DOI:
Current Issue | Archive | Adv Search |
STUDIES OF PHASE RELATIONS BETWEEN MISCHMETAL (Mm) AND MmNi_5 TOGETHER WITH THEIR HYDROGEN ABSORPTION PROPERTIES
CHE Guangcan; LIANG Jingkui; YU Yude (Institute of Physics; Academia Sinica; Beijing)
Cite this article: 

CHE Guangcan; LIANG Jingkui; YU Yude (Institute of Physics; Academia Sinica; Beijing). STUDIES OF PHASE RELATIONS BETWEEN MISCHMETAL (Mm) AND MmNi_5 TOGETHER WITH THEIR HYDROGEN ABSORPTION PROPERTIES. Acta Metall Sin, 1986, 22(5): 106-111.

Download:  PDF(453KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  X-ray diffraction, DTA and other methods were used to determine the phase relations between native mischmetal (Mm) and MmNi_5 as well as the phase diagram of LaNi_5-PrNi_5 pseudo-binary system. The hydrogen desorption capacities and hydrogen adsorption plateau pressure of LaNi_5-PrNi_5 (CeNi_5, NdNi_5) system varied with the compositions of specimens and the hydrogen absorption properties of La-rich and Ce-rich MmNi_5 were also studied. The free energy, △Z, the enthalpy, △H, and the entropy, △S, of the hydride of La-rich MmNi_5 were estimated to be 6.14 kJ/mol H_2,-20.92 kJ/mol H_2 and-90.8 J/K.mol H_2 respectively.
Received:  18 May 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I5/106

1 车广灿;俞育德;梁敬魁,物理学报,33(1984) ,770.
2 梁敬魁;王朝果,金属学报,18(1982) ,592.
3 Che Guangcan (车广灿), Proc. of Beijing Int. Symp. on Hydrogen Systems, Pergamon Press New York, 1985. p. 56.
No related articles found!
No Suggested Reading articles found!