Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (5): 146-148    DOI:
Current Issue | Archive | Adv Search |
FURTHER DEVELOPMENT OF ADIABATIC CALORIMETER FOR PRECISELY MEASURING ELECTRIC RESISTIVITY OF KARMA ALLOY FROM 70 TO 440 K
TAN Zhicheng; WANG Zhuang (Dalian Institute of Chemical Physics; Academia Sinica)
Cite this article: 

TAN Zhicheng; WANG Zhuang (Dalian Institute of Chemical Physics; Academia Sinica). FURTHER DEVELOPMENT OF ADIABATIC CALORIMETER FOR PRECISELY MEASURING ELECTRIC RESISTIVITY OF KARMA ALLOY FROM 70 TO 440 K. Acta Metall Sin, 1986, 22(5): 146-148.

Download:  PDF(207KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The precise measurement of electrical resistivity of Karma alloy in the temperature range from 70 to 440 K was conducted in the further development of an adiabatic calorimeter. The minimum and maximum resistivity was obtained as 133.340 and 133.906 μΩcm respectively. A maximum near 340 K on the plot of temperature dependence upon resistivity is an anomaly that seems to be neceessary for any further study.
Received:  18 May 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I5/146

1 谭志诚;周立幸;陈淑霞;尹安学;孙毅;叶锦春;王秀坤,中国科学,B辑,(1983) ,№6,497.
2 1964 Book of ASTM Standards, 8, Publ. ASTM, 1964, p. 196.
3 中国国家标准汇编,No.8,中国标准出版社,1984,p.774.
4 Furukawa, G.T.; Reilly, M.L.; Saba, W.G., NBS Special Publlication 300-Vol.6, Precision Measurement and Calibration, Selected NBS Paper on Heat, Ed. Ginnings, D.C., U.S. Government Printing office, Washington, D.C. 1970, P. 110
No related articles found!