| FURTHER DEVELOPMENT OF ADIABATIC CALORIMETER FOR PRECISELY MEASURING ELECTRIC RESISTIVITY OF KARMA ALLOY FROM 70 TO 440 K |
| TAN Zhicheng; WANG Zhuang (Dalian Institute of Chemical Physics; Academia Sinica) |
|
Cite this article:
TAN Zhicheng; WANG Zhuang (Dalian Institute of Chemical Physics; Academia Sinica). FURTHER DEVELOPMENT OF ADIABATIC CALORIMETER FOR PRECISELY MEASURING ELECTRIC RESISTIVITY OF KARMA ALLOY FROM 70 TO 440 K. Acta Metall Sin, 1986, 22(5): 146-148.
|
|
|
Abstract The precise measurement of electrical resistivity of Karma alloy in the temperature range from 70 to 440 K was conducted in the further development of an adiabatic calorimeter. The minimum and maximum resistivity was obtained as 133.340 and 133.906 μΩcm respectively. A maximum near 340 K on the plot of temperature dependence upon resistivity is an anomaly that seems to be neceessary for any further study.
|
|
Received: 18 May 1986
|
1 谭志诚;周立幸;陈淑霞;尹安学;孙毅;叶锦春;王秀坤,中国科学,B辑,(1983) ,№6,497. 2 1964 Book of ASTM Standards, 8, Publ. ASTM, 1964, p. 196. 3 中国国家标准汇编,No.8,中国标准出版社,1984,p.774. 4 Furukawa, G.T.; Reilly, M.L.; Saba, W.G., NBS Special Publlication 300-Vol.6, Precision Measurement and Calibration, Selected NBS Paper on Heat, Ed. Ginnings, D.C., U.S. Government Printing office, Washington, D.C. 1970, P. 110 |