Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (6): 139-141    DOI:
Current Issue | Archive | Adv Search |
A METHOD FOR SIMULTANEOUS DETERMINATION OF Ce SUB-GROUP AND Y IN Ni-BASE ALLOY OR STEEL
by SUN Ruocheng; MA Yushan (Institute of Metal Research; Academia Siniea; Shenyang)
Cite this article: 

by SUN Ruocheng; MA Yushan (Institute of Metal Research; Academia Siniea; Shenyang). A METHOD FOR SIMULTANEOUS DETERMINATION OF Ce SUB-GROUP AND Y IN Ni-BASE ALLOY OR STEEL. Acta Metall Sin, 1986, 22(6): 139-141.

Download:  PDF(215KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new method for the simultaneous determination of the Ce subgroup and Y in Ni-base alloy or steel was developed. The trouble to analysis from the mutual overlap on the spectra resulted by the complexes of Ce sub-group and Y with chlorophosphonazo-P-NO_2 in HClO_4 has been relieved by complete separation using first derivative spectrophotometry. The interference of foreign ions can be eliminated by masking with VC, Zn-EDTA and NH_4F. The method has been applied to Ni-base alloy or steel containing 0.05—0.4% Ce sub-group and Y with a relative error ±8%.
Received:  18 June 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I6/139

1 潘教麦,化学试剂,(1981) ,№ 4,48。
2 孙慧芳;潘教麦;黄留庆,理化检验,19 (1983) ,№ 1,11。
3 马玉珊,冶金分析,待发表。
4 孙若诚,稀有金属,8 (1984) ,№ 1,56。
No related articles found!
No Suggested Reading articles found!