Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (1): 146-148    DOI:
Current Issue | Archive | Adv Search |
ON THE CRYSTALLIZATION OF ELECTRODEPOSITED AMORPHOUS Ni-P ALLOY
ZHAO Zhongyong YAO Jinjun FU Bin (Wuhan Research Institute of Materials Protection)
Cite this article: 

ZHAO Zhongyong YAO Jinjun FU Bin (Wuhan Research Institute of Materials Protection). ON THE CRYSTALLIZATION OF ELECTRODEPOSITED AMORPHOUS Ni-P ALLOY. Acta Metall Sin, 1987, 23(1): 146-148.

Download:  PDF(179KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Four exothermal peaks at 280,310,343 and 410℃ are revealed on the crystallization of the electrodeposited amorphous Ni_(75)P_(25) film examined by DTA.X-ray diffraction shows that the exothermal peak at 310℃ corresponds with the phase transformation from the meta- stable phase α to ones α_1,α_2 and α_3,and peak at 343℃ is related to the adjustment of α_1, α_2 and α_3 each other.
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/146

1 Bagley B G.Turnbull D.J Appl Phys,1968;39:5681
2 郭可信,梁金忠,孟宪英等.物理学报,1982,31:988
3 梁金忠,赖宗和,吴玉琨等,物理学报,1984;33:1037
4 赖宗和,吴玉琨,郭可信.物理学报,1984;33:1182
5 增井宽二,山田敏夫,久松,金属表面技术,1980;32(8) :28-34N
No related articles found!
No Suggested Reading articles found!