| ON THE CRYSTALLIZATION OF ELECTRODEPOSITED AMORPHOUS Ni-P ALLOY |
| ZHAO Zhongyong YAO Jinjun FU Bin (Wuhan Research Institute of Materials Protection) |
|
Cite this article:
ZHAO Zhongyong YAO Jinjun FU Bin (Wuhan Research Institute of Materials Protection). ON THE CRYSTALLIZATION OF ELECTRODEPOSITED AMORPHOUS Ni-P ALLOY. Acta Metall Sin, 1987, 23(1): 146-148.
|
|
|
Abstract Four exothermal peaks at 280,310,343 and 410℃ are revealed on the crystallization of the electrodeposited amorphous Ni_(75)P_(25) film examined by DTA.X-ray diffraction shows that the exothermal peak at 310℃ corresponds with the phase transformation from the meta- stable phase α to ones α_1,α_2 and α_3,and peak at 343℃ is related to the adjustment of α_1, α_2 and α_3 each other.
|
|
Received: 18 January 1987
|
1 Bagley B G.Turnbull D.J Appl Phys,1968;39:5681 2 郭可信,梁金忠,孟宪英等.物理学报,1982,31:988 3 梁金忠,赖宗和,吴玉琨等,物理学报,1984;33:1037 4 赖宗和,吴玉琨,郭可信.物理学报,1984;33:1182 5 增井宽二,山田敏夫,久松,金属表面技术,1980;32(8) :28-34N |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|