Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (2): 111-117    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF FERRITE-MARTENSITE MICROSTRUCTURE ON STRESS AND STRAIN DISTRIBUTIONS IN TWO PHASES FOR 12CrMo STEEL ANALYSED WITH FINITE ELEMENT METHOD
LI Zhonghua; LUO Jinghua; WANG Yonglan; KUANG Zhenbang; SHAO Tanhua; ZHOU Huijiu (Xi'an Jiaotong University) (Manuscript received 12 May; 1985; revised manuscript 5 May; 1986)
Cite this article: 

LI Zhonghua; LUO Jinghua; WANG Yonglan; KUANG Zhenbang; SHAO Tanhua; ZHOU Huijiu (Xi'an Jiaotong University) (Manuscript received 12 May; 1985; revised manuscript 5 May; 1986). INFLUENCE OF FERRITE-MARTENSITE MICROSTRUCTURE ON STRESS AND STRAIN DISTRIBUTIONS IN TWO PHASES FOR 12CrMo STEEL ANALYSED WITH FINITE ELEMENT METHOD. Acta Metall Sin, 1987, 23(2): 111-117.

Download:  PDF(630KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By use of a computer program, the finite element method has been employed to calculated the effect of particle size, matrix and volume fraction of phases on the stress and strain distributions in 12CrMo ferrite-martensite steel. In particular, the distributions of hydrostatic stress and maximum shear stress in each phase are given. The microscopic fracture mechanism revealed by these stress distributions coincides with experimental observations.
Received:  18 February 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I2/111

1 Sundstroem B O. Mater Sci Eng 1973; 12 (5/6) : 265
2 Ankem S, Margolin H. Metall Trans A 1982; 13: 603
3 Fischmeister H, Karlsson B. Z Metallk 1977; 68 (5) : 311
4 Karlsson B, Sundstroem B O. Mater Sci Eng 1974; 16: 161
5 李中华,王永兰,罗景华,匡震邦,邵谭华,周惠久,金属学报,1987;23
6 王永兰,邵谭华,耿泽峻,刘德跃,西安交通大学学报,1984;18(6) :77
7 Kuntio T, Shimizu M, Yamada K. Fracture Mechanics of Ductile and Tough Materials Applications to Energy Related Structure.1981,221
No related articles found!
No Suggested Reading articles found!