| KINETICS OF OXIDATION LEACHING OF Ag IN AMMONIACAL SOLUTIONS |
| MENG Xinghui; KE Jiajun(Institute of Chemical Metallurgy; Academia Sinica; Beijing)(Manuscript received 23 June; 1985; revised manuscript 17 February; 1986) |
|
Cite this article:
MENG Xinghui; KE Jiajun(Institute of Chemical Metallurgy; Academia Sinica; Beijing)(Manuscript received 23 June; 1985; revised manuscript 17 February; 1986). KINETICS OF OXIDATION LEACHING OF Ag IN AMMONIACAL SOLUTIONS. Acta Metall Sin, 1987, 23(2): 190-197.
|
|
|
Abstract The leaching behaviour of Ag in NH_3-O_2 and NH_3-H_2O_2 aqueous solutions was investigated. The results show that the dissolution of Ag was restrained by forming of a silver suboxide film on the surface under low oxidant concentration and atmospheric pressure conditions (e.g., in NH_3-O_2-H_2O system); when the concentration of oxidant was high enough (e.g., in NH_3-H_2O_2-H_2O system), the leaching process was carried out without forming of the film and the rate of dissolution of Ag was controlled by a step of mass transfer. Based on experimental results, a reaction mechanism of oxidation leaching of Ag in ammoniacal solutions was discussed.
|
|
Received: 18 February 1987
|
1 柯家骏,涂桃枝,卞直旭.吉林冶金,1983;(2) :28 2 柯家骏,岳良东,金属学报 1984;20:A197 3 Hofmann K A, Hofmann U. Ber Dtsch Chem Ges, 1928; 61: 2566 4 Kakovskii I A, Tyurin N G. Doklady Akad Nauk SSSR 1960; 130: 821 5 梅津良之,户沢一光,佐佐木金一,日本鉱業会誌,1971;87:29 6 Grybos R, Samotus A. J Less-Common Met, 1982; 84: 307; 1983; 91:61 7 岳良东,柯家骏.有色金属1983;35(1) :76 8 蒙星辉,中国科学院化工冶金研究所硕士论文,1984 9 Levich V G. Physicochemical Hydrodynamics. Englewood Cliffs, N. J.: Prentice-Hall, 1962; 60-7 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|