Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (2): 190-197    DOI:
Current Issue | Archive | Adv Search |
KINETICS OF OXIDATION LEACHING OF Ag IN AMMONIACAL SOLUTIONS
MENG Xinghui; KE Jiajun(Institute of Chemical Metallurgy; Academia Sinica; Beijing)(Manuscript received 23 June; 1985; revised manuscript 17 February; 1986)
Cite this article: 

MENG Xinghui; KE Jiajun(Institute of Chemical Metallurgy; Academia Sinica; Beijing)(Manuscript received 23 June; 1985; revised manuscript 17 February; 1986). KINETICS OF OXIDATION LEACHING OF Ag IN AMMONIACAL SOLUTIONS. Acta Metall Sin, 1987, 23(2): 190-197.

Download:  PDF(640KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The leaching behaviour of Ag in NH_3-O_2 and NH_3-H_2O_2 aqueous solutions was investigated. The results show that the dissolution of Ag was restrained by forming of a silver suboxide film on the surface under low oxidant concentration and atmospheric pressure conditions (e.g., in NH_3-O_2-H_2O system); when the concentration of oxidant was high enough (e.g., in NH_3-H_2O_2-H_2O system), the leaching process was carried out without forming of the film and the rate of dissolution of Ag was controlled by a step of mass transfer. Based on experimental results, a reaction mechanism of oxidation leaching of Ag in ammoniacal solutions was discussed.
Received:  18 February 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I2/190

1 柯家骏,涂桃枝,卞直旭.吉林冶金,1983;(2) :28
2 柯家骏,岳良东,金属学报 1984;20:A197
3 Hofmann K A, Hofmann U. Ber Dtsch Chem Ges, 1928; 61: 2566
4 Kakovskii I A, Tyurin N G. Doklady Akad Nauk SSSR 1960; 130: 821
5 梅津良之,户沢一光,佐佐木金一,日本鉱業会誌,1971;87:29
6 Grybos R, Samotus A. J Less-Common Met, 1982; 84: 307; 1983; 91:61
7 岳良东,柯家骏.有色金属1983;35(1) :76
8 蒙星辉,中国科学院化工冶金研究所硕士论文,1984
9 Levich V G. Physicochemical Hydrodynamics. Englewood Cliffs, N. J.: Prentice-Hall, 1962; 60-7
No related articles found!
No Suggested Reading articles found!