Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (3): 200-310    DOI:
Current Issue | Archive | Adv Search |
TEM INVESTIGATION ON MICROSTRUCTURE AND FRACTURE PROCESS OF A PEARLITIC STEEL
HUANG Xiaoying; GUO Wei; PAN Tianxi; ZHAO Jian (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beiling) (Manuscript received 29 July; 1985; revised manuscript 29 February; 1986)
Cite this article: 

HUANG Xiaoying; GUO Wei; PAN Tianxi; ZHAO Jian (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beiling) (Manuscript received 29 July; 1985; revised manuscript 29 February; 1986). TEM INVESTIGATION ON MICROSTRUCTURE AND FRACTURE PROCESS OF A PEARLITIC STEEL. Acta Metall Sin, 1987, 23(3): 200-310.

Download:  PDF(3268KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructure and fracture process of an eutectoid pearlitic steel have been observated and analysed by means of electron-diffraction-contrast technique and SEM. The fine structure of ferrite and cementite as well as the character of interface combination between the two phases in pearlite have been studied. The fracture process, which is characterized by layer structure was discussed in the term of crystallography. To evaluate the toughness level of pearlitie steels, a new macro-parameter, size of SOCC group, has been suggested.
Received:  18 March 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I3/200

1 Darken L S, Fisher R M. In: Zackay V F, Aaronson H I. eds., Decompsition of Austenite by Diffusional Processes, New York: Interscience, 1962: 249-294
2 Lupton D F, Warrington D H. Acta Metall, 1972; 20: 1325
3 Park Y J, Bernstein I M. In: Taplined D M R. ed. Proc. of Fouth Int. Conf, on Fracture, Vol. 2. Waterloo. Canada: Univ, of Waterloo Press, 1977: 33-40
4 赵坚,朱桂兰。理化检验,物理分册,1982;18(3) :47
5 Hyzak J M, Bernstein I M,. Metall Trans, 1976; 74: 1217-1224
6 黄孝瑛,透射电子显微学,第11章,上海科学出版社,1987.
No related articles found!
No Suggested Reading articles found!