Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (3): 257-261    DOI:
Current Issue | Archive | Adv Search |
ELECTRODE PROCESS OF ELECTROLYTIC COATING OF Al IN FUSED NaCl-KCl SALT BATH
MA Zhangyuan; XU Zhiqiang; CAO Tieliang; SHI Shengtai (Shih Shing-Tai)(Shanghai Institute of Metallurgy; Academis Sinica) (Manuscript received 22 July; 1984; revised manuscript 26 November; 1985)
Cite this article: 

MA Zhangyuan; XU Zhiqiang; CAO Tieliang; SHI Shengtai (Shih Shing-Tai)(Shanghai Institute of Metallurgy; Academis Sinica) (Manuscript received 22 July; 1984; revised manuscript 26 November; 1985). ELECTRODE PROCESS OF ELECTROLYTIC COATING OF Al IN FUSED NaCl-KCl SALT BATH. Acta Metall Sin, 1987, 23(3): 257-261.

Download:  PDF(350KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The standard oxidation/reduction potential of Al including its valence state in fused salt was examined, The anodic dissolution of Al can be shown by the equation Al→Al~3+3e. The standard oxidation/reduction potential of Al in fused salt is-1.122V as obtained by graphical method. Cathodic process has been investigated by means of steady state method. Separate potentials of some ions, the coefficient of diffusion ,of AlCl_4~- ion and kinetic constants of Al ion reduction have been meastured and discussed.
Received:  18 March 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I3/257

1 石声泰 (Shin S T). In: Rapp R A ed., High Temperature Corrosion, NACE-6, 1983: 460
2 石声泰.中国腐蚀与防护学报,1981;1(3) :1-7
3 石声泰,冯明仁,曹铁梁,马樟源,张彩玲.中国腐蚀与防护学报,1981;1(4) :1-7
4 Shin S T (石声泰), Feng M R (冯明仁), Cao T L (曹铁梁), Zhang C L (张彩玲). In: Metallic Corrosion, Proceedings 8th International Congress on Metallic Corrosion, 1981, Vol. Ⅱ, Deutsche Gesellschaft fur Chemisches Apparalewesen e. v. Frankfurt am Main, 1981: 1127
5 Winter D G, Strachan A M. In: Jones M J. Advances in Extractive Metallurgy, An Int. Symp. Organized by the Institution Metallurgy, London: Inst. Mining and Metall., 1977: 177
No related articles found!