Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (3): 293-295    DOI:
Current Issue | Archive | Adv Search |
MOSSBAUER EFFECT STUDY OF Nd_(15)(Fe_1-xCox)_(77)B_8
WANG Huaiyu; ZENG Xunyi(Shanghai Institute of Metallugy; Academia Sinica) (Manuscript received 25 October 1985: revised manuscript 28 May; 1986)
Cite this article: 

WANG Huaiyu; ZENG Xunyi(Shanghai Institute of Metallugy; Academia Sinica) (Manuscript received 25 October 1985: revised manuscript 28 May; 1986). MOSSBAUER EFFECT STUDY OF Nd_(15)(Fe_1-xCox)_(77)B_8. Acta Metall Sin, 1987, 23(3): 293-295.

Download:  PDF(212KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Hyperfine parameters of Fe sublattices in Nd_2Fe_(14)B have been deduced by refering to the magnetic moment values of Fe for different sites obtained by Givord et al using polarized neutron diffraction technique. By examining the ~(57)Fe Mǒssbauer spectra of Co doped specimen, it is observed that Co atoms, while their amount is small, preferentially enter k_2 site of Fe and thus creat unequivalent sites of their nearest neighbors, e. g. k_1 and j_2 Fesites. And they will enter other Fe-site if more Co was doped.
Received:  18 March 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I3/293

1 Sagawa M, Fujimura S, Togawa M et al. J Appl Phys, 1984; 55: 2083
2 Matsuura Y, Hirosawa S, Yamamoto H et at. Appl Phys Letter, 1985; 46: 308
3 Spada F, Abache C, Oesterreicher H. J Less-Common Met, 1984; 99: L21
4 李正文等.科学研究论文集-穆斯堡尔谱的计算机拟合技术,北京钢铁学院编,1984:152
5 Herbst J F, Croat J J, Pinkerton F E, Yelon W B phys Rev 1984; B29: 4176
6 Pinkerton P E, Dunham W R. Appl Phys Letter, 1984; 45: 1248
7 Onodera H, Yamaguchi Y, Yamamoto H et al. J Magn Magn Mater, 1984; 46: 151
8 Givord D, Li H S, Tasset F. J Appl Phys, 1985; 57: 4100
9 Ping Jueyun, Li Zhengwen, Ma Ruzhang et at. In: Xu Guangxian, Xiao Jlmei ed., New Frontiers in RE Science and Application, Vol. 2, China Beijing: Science Press, 1985: 982
No related articles found!