| MOSSBAUER EFFECT STUDY OF Nd_(15)(Fe_1-xCox)_(77)B_8 |
| WANG Huaiyu; ZENG Xunyi(Shanghai Institute of Metallugy; Academia Sinica) (Manuscript received 25 October 1985: revised manuscript 28 May; 1986) |
|
Cite this article:
WANG Huaiyu; ZENG Xunyi(Shanghai Institute of Metallugy; Academia Sinica) (Manuscript received 25 October 1985: revised manuscript 28 May; 1986). MOSSBAUER EFFECT STUDY OF Nd_(15)(Fe_1-xCox)_(77)B_8. Acta Metall Sin, 1987, 23(3): 293-295.
|
|
|
Abstract Hyperfine parameters of Fe sublattices in Nd_2Fe_(14)B have been deduced by refering to the magnetic moment values of Fe for different sites obtained by Givord et al using polarized neutron diffraction technique. By examining the ~(57)Fe Mǒssbauer spectra of Co doped specimen, it is observed that Co atoms, while their amount is small, preferentially enter k_2 site of Fe and thus creat unequivalent sites of their nearest neighbors, e. g. k_1 and j_2 Fesites. And they will enter other Fe-site if more Co was doped.
|
|
Received: 18 March 1987
|
1 Sagawa M, Fujimura S, Togawa M et al. J Appl Phys, 1984; 55: 2083 2 Matsuura Y, Hirosawa S, Yamamoto H et at. Appl Phys Letter, 1985; 46: 308 3 Spada F, Abache C, Oesterreicher H. J Less-Common Met, 1984; 99: L21 4 李正文等.科学研究论文集-穆斯堡尔谱的计算机拟合技术,北京钢铁学院编,1984:152 5 Herbst J F, Croat J J, Pinkerton F E, Yelon W B phys Rev 1984; B29: 4176 6 Pinkerton P E, Dunham W R. Appl Phys Letter, 1984; 45: 1248 7 Onodera H, Yamaguchi Y, Yamamoto H et al. J Magn Magn Mater, 1984; 46: 151 8 Givord D, Li H S, Tasset F. J Appl Phys, 1985; 57: 4100 9 Ping Jueyun, Li Zhengwen, Ma Ruzhang et at. In: Xu Guangxian, Xiao Jlmei ed., New Frontiers in RE Science and Application, Vol. 2, China Beijing: Science Press, 1985: 982 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|