THE CRITICAL STRESS OF FATIGUE CRACK INITIATION FOR MEDIUM CARBON STEEL
by LIN Jizhong; LIU Shuhua; WU Yushu; LI Yi (China Academy of Railway Sciences) (Manuscript received 22 April; 1986; revised manuscript 25 August; 1986)
Cite this article: 

by LIN Jizhong; LIU Shuhua; WU Yushu; LI Yi (China Academy of Railway Sciences) (Manuscript received 22 April; 1986; revised manuscript 25 August; 1986). THE CRITICAL STRESS OF FATIGUE CRACK INITIATION FOR MEDIUM CARBON STEEL. Acta Metall Sin, 1987, 23(4): 339-340.

Download:  PDF(118KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Notch fracture machanics was used to investigate the fatigue crack initiation from the notch tip for medium carbon steels (0.4-0.6 wt-%C). The relationships between the maximum stress range at the notch root, △σ_(max), and the number of cycles before fatigue crack initiation, N_i, have been determined. Furthermore, the threshold stress of fatigue crack initiation, △σ_(max)th, as a function of C content or of yield strength of the steel has been proposed.
Received:  18 April 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I4/339

No related articles found!
No Suggested Reading articles found!