COMPOSITION DESIGN AND EXPERIMENTAL STUDY OF SINGLE CRYSTAL ALLOY DD3
by WU Zhongtang; WEN Zhongyuan; CHEN Dehou (Institute of Aeronautical Materials; Beijing) (Manuscript received 19 June; 1985; revised manuscript 27 January; 1986)
Cite this article: 

by WU Zhongtang; WEN Zhongyuan; CHEN Dehou (Institute of Aeronautical Materials; Beijing) (Manuscript received 19 June; 1985; revised manuscript 27 January; 1986). COMPOSITION DESIGN AND EXPERIMENTAL STUDY OF SINGLE CRYSTAL ALLOY DD3. Acta Metall Sin, 1987, 23(4): 349-356.

Download:  PDF(1192KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Orthogonal design calculation of the composition of single crystal has been carried out using the method proposed by Watanabe. The effects of individual elements on the volume fraction of γ' phase, the electron vacancy number and the lattice parameters of γ and γ' phase as well as the lattice misfit between γ matrix and γ' precipitate have been predicted. Based on the calculation, the dependance of composition on microstructure and mechanical properties has been proposed and compared with experimental results. The composition designed by present provides about 60% of volume fraction of γ' in the alloy, good structural tability excellent high temperature mechanical properties were obtained.
Received:  18 April 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I4/349

1 Erickson J S, Owczarski W A, Curran P M. Met Prog, 1971; 99(3) :58
2 Versnyder F L, Shank M E. Mater Sci Eng, 1970; 6:213
3 Jackson J J, Donachie M J, Henricks R J, Gell M. Met Trans, 1977; 8A:1615
4 Gell M, Duhl D N, Giamei A F. In:Tien J K et al. eds., Proc 4th Int Symp on Superalloys, Metals Park, ASM, 1980:205
5 Strangman T E, Hoppin G S Ⅲ, Phipps C M, Harris K, Schwer R E. In:Tien J K et al. eds., Superalloys, Proc 4th Int Symp on Superalloys, Metals Park, ASM, 1980:215
6 杨洪才.金属学报,1982;18:510
7 青木晃,野田俊治,村田纯教,汤川夏夫,鉄鋼,1982;68:s1346
8 #12
9 渡辺力藏,九重常男,铁鋼,1975;61(9) :2274
10 Decker R F. Strengthening Mechanisms in Nickel Base Superalloys, Symposium: Steel Streng-thing Mechanisms, Zurich, 1969, Greenwich: Climax Molybdenum, 1970:147
11 Woodyatt L R, Sims C T, Beattie H J Jr. Trans AIME, 1966; 236:519
12 原田広史,山崎道夫,铁鋼,1979;(7) :1059-1068
13 Aldred P. S A E 75104
No related articles found!
No Suggested Reading articles found!