CONSTRUCTION OF MOLTEN SALT PHASE DIAGRAMS BY COMBINATION OF CALCULATION WITH MEASUREMENT
by QIAO Zhiyu; DUAN Shuzhen; GUI Weizhen; SUN Minsheng (Beijing University of Iron and Steel Technology) (Manuscript received 31 March; 1986; revised manuscript 24 November; 1986)
Cite this article: 

by QIAO Zhiyu; DUAN Shuzhen; GUI Weizhen; SUN Minsheng (Beijing University of Iron and Steel Technology) (Manuscript received 31 March; 1986; revised manuscript 24 November; 1986). CONSTRUCTION OF MOLTEN SALT PHASE DIAGRAMS BY COMBINATION OF CALCULATION WITH MEASUREMENT. Acta Metall Sin, 1987, 23(4): 357-362.

Download:  PDF(475KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The principle and mathods of calculation of phase diagram, especially the geometric models for determination of excess molar Gibbs energy and excess partial molar Gibbs energy in all phases have been reviewed. Considering the significance and the limitation of calculation of phase diagram, it is pointed out that the combination of calculation with measurement is the best method for construction of molten salt phase diagrams. The procedure of this method have also been described.
Received:  18 April 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I4/357

1 CALPHAD Jounral, Pergamon, 1977-1987
2 Pelton A D. AIME Conference Proceedings, Toronto Canada, 1986或:稀有金属 (国际),1987; 6 (1) : 54; (2) : 117
3 Hillerr M.在北京钢铁学院的讲稿,北京1980
4 乔芝郁,Hillert M.北京钢铁学院学报,1981;(1) :109,1981;(3) :77
5 乔芝郁, Hillert M. CALPHAD J, 1985; 9(2) :143
6 Eriksson G. Acta Chem Scand, 1971; 25:2651
7 Eriksson G. Chem Scr, 1975; 8:100
8 Besmann T M. Oak Ridge National Lab Oak Ridge Report ORNLTM, 1977:5575
9 郭祝崑等,1984年全国第三届相图学术会议论文汇编,第一册,昆明,1984
10 Pelton D,乔芝郁,私人通讯
11 乔芝郁.见:段淑贞,乔芝郁主编,熔盐物理化学和电化学,北京:冶金工业出版社,(待发表)
12 李瑞青,乔芝郁,段淑贞,周国治,北京钢铁学院学报,1987;(3)
13 Hillert M. CALPHAD J, 1980; 4(1) :1
14 乔芝郁,莫雯静,武世民,朱元凯,稀有金属(国际版),1983;2(2) :163
15 周国治,CALPHAD J,1987;11(2) 183
16 陈征宇,周国治.1986年全国第四届相图学术会议论文汇编,长沙,1986
17 Qiao Zhiyu (乔芝郁). Sangster J, Pelton A D. CALPHAD J, 1987; 11(4)
18 李瑞青,乔芝郁,段淑贞,周国治.1986年全国第四届相图学术会议论文汇编,长沙,1986
No related articles found!
No Suggested Reading articles found!