FORMATION MECHANISM OF BUTTERFLY MARTENSITE
by GONG Hai (Dalian Institute of Railway); GU Nanju (Hebei Technological Institute; Shijiazhuang)(Manuscript received 28; February;1986)
Cite this article: 

by GONG Hai (Dalian Institute of Railway); GU Nanju (Hebei Technological Institute; Shijiazhuang)(Manuscript received 28; February;1986). FORMATION MECHANISM OF BUTTERFLY MARTENSITE. Acta Metall Sin, 1987, 23(5): 374-379.

Download:  PDF(1826KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The butterfly martensite formed in T12A, GCr18Mo, CrMn and 25Cr2Ni-4WA (carburized) steels have been examined using optical microscopy and TEM. It was found that the mid-rib of butterfly martensite is a thin plate martensite and the formation of butterfly martensite is not a continuous process, but rather a compound one consisting of some separated stages. In the initial stage, the crossed or kinked thin plate martensite forms, and then it grows toward cross-range into the butterfly martensite with or without tail.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/374

1 梅本実,田村今男.水曜会誌,1980;119:281
2 贡海,苏东升.金属热处理,1983;(1) :32
3 纪芬,贡海.理化检验(物理分册),1985;21(5) :11
4 梅本実,渡井康之,田村今男.日本金属学会会誌,1980;44:453
5 Brook R, Entwisle A R. J Iron Steel Inst. 1965; 203: 905
6 Umemoto M, Tamura I. Proc of ICOMAT-79, Cambridge (USA), 1979: 53
7 Tamura I. Proc of ICOMAT-76, Kobe(Japan), 1976: 5
No related articles found!
No Suggested Reading articles found!