Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (5): 434-436    DOI:
Current Issue | Archive | Adv Search |
CREEP FRICTION STRESS OF γ' STRENGTHENED Ni-BASE SUPERALLOYS
by YANG Zhi'an; XIAO Yaotian; SHI Changxu(C. H. Shih) (Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 10 Octorber; 1985; revised manuscript 22 Appril; 1986)
Cite this article: 

by YANG Zhi'an; XIAO Yaotian; SHI Changxu(C. H. Shih) (Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 10 Octorber; 1985; revised manuscript 22 Appril; 1986). CREEP FRICTION STRESS OF γ' STRENGTHENED Ni-BASE SUPERALLOYS. Acta Metall Sin, 1987, 23(5): 434-436.

Download:  PDF(229KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The creep friction stress of γ' strengthened superalloys containing 5 and 10 wt-% Co has been measured by means of stress dip test on the creep machine modified by the authors. The results analized with either asymptote or McLean's method show that Co will linearly increase the friction stress value for Ni-base superalloys.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/434

1 Lund R W, Nix W D. Acta Metall, 1976; 24: 469
2 Ajaja O. Howson T E, Purushothaman S, Tien J K. Mater Sci. Eng, 1980; 44: 165
3 阳志安,肖耀天,师昌绪,金属学报.1983;19:A300
4 Lagneborg R. J Mater Sci, 1968; 3: 596
5 Threadgill P L, Wilshire B. Creep Strength in Steel and High-Temperature Alloys, ISI, Sheffield, 1972, London: Metals Society 1974
6 Williams K R, Wilshire B. Met Sci J, 1973: 7: 176
7 Williams K R, Wilshire B. Mater Sci Eng, 1977; 28: 289
8 McLean M. Scr Metall, 1979; 13: 339
9 McLean M. Proc R Soc London, 1980; A371: 279
10 Friedel J. Dislocations, Oxford: Pergamon, 1964: 239
11 Yang Z A, Xiao Y T, Shih C H. High Temperature Technique, 1987; (2)
12 阳志安.博士论文,中国科学院金属研究所,1985
13 Yang Z A, Xiao Y T, ShihCH. In,Proc Int Conf on Creep' 86, Tokyo, 1986
14 Stevens R A, Flewitt P E J. Acta Met all, 1981; 29: 867
No related articles found!