EFFECT OF OXYGEN CONTENT ON STRUCTURAL DISTORTION AND SUPERCONDUCTIVITY OF Y-Ba-Cu-O SYSTEM
by QI Hongbo; ZHU Naiping; PANG Dexing; JIANG Xiaoping; YU Huafeng;QIAO Guiwen (Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 30 April; 1987)
Cite this article: 

by QI Hongbo; ZHU Naiping; PANG Dexing; JIANG Xiaoping; YU Huafeng;QIAO Guiwen (Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 30 April; 1987). EFFECT OF OXYGEN CONTENT ON STRUCTURAL DISTORTION AND SUPERCONDUCTIVITY OF Y-Ba-Cu-O SYSTEM. Acta Metall Sin, 1987, 23(5): 444-446.

Download:  PDF(221KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The cooling rate results in the change of structural distortion of Y_1Ba_2Cu_3O_(9-x) phase, which depends upon the oxygen content in it. Y_1Ba_2Cu_3O_(9-x) phase reacts with O_2 in 600-400℃ during cooling, this causes the structural distortion related to superconductivity. Slow cooling in this temperature range benefits the absorption of O_2.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/444

1 朱乃平,江晓平,庞德兴,漆洪波,苏国跃,张泽,杨中进,俞华锋.金属学报,1987;23 A250
2 Beyers R, Lim G, Rngler E M, Savoy R J, Shaw T M, Dinger T R, Gallagher W J, Sandstrom R L. Submitted to Applied Physics Letters
3 Jiang Xiaoping, Yu Huafeng, Zhang Ze, Zhu Naiping, Qi Hongbo, Yang Zhong jin. Submitted to Applied Physics Letters
No related articles found!