Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (6): 503-506    DOI:
Current Issue | Archive | Adv Search |
SOLID SOLUBILITIES OF Ce AND Nd IN α-Fe
by ZHANG Fuzhong; GU Lijun; OU Liuxing; LIU Woyuan; YAN Yuxin (Baotou Rare Earth Research Institute) (Manuscript received 25 September; 1986)
Cite this article: 

by ZHANG Fuzhong; GU Lijun; OU Liuxing; LIU Woyuan; YAN Yuxin (Baotou Rare Earth Research Institute) (Manuscript received 25 September; 1986). SOLID SOLUBILITIES OF Ce AND Nd IN α-Fe. Acta Metall Sin, 1987, 23(6): 503-506.

Download:  PDF(312KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Solid solubilities of Ce and Nd in α-Fe were determined with the aid of X-ray diffraction lattice parameter measurements and electron-microprobe quantitative analysis. The alloys were prepared by vacuum levitation melting using 99.987wt-%Fe, 99.9wt-%Ce and 99.95wt-%Nd, respectively. They were subsequently homogenized at 1200℃, then cooled down to room temperature to achieve quasi-equilibrium conditions. Solubilities of 0.048 wt-%Ce and 0.055 wt-% Nd in α-Fe were obtained.
Received:  18 June 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I6/503

1 Jepson J O, Duwez P. Trans ASM, 1955; 47: 543-553
2 Richerd J. Mem Sci Roy Metall, 1962; 59: 527
3 Haefling J F, Daane AH. In: Spedding F H, Daane A H eds., The Rare Earth, New York: Wiley, 1961: 280
4 #12
5 庄应烘,荣国器,唐晓峰.中国稀土学报,1983;1(1) :58-61
6 #12
7 Domagala R F, Rausch J J, Levinson D W. Trans ASM, 1961; 53: 137-155
8 颜玉新,章复中.稀有金属(季刊),1987;6(2) :131
9 #12
No related articles found!