Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (6): 527-530    DOI:
Current Issue | Archive | Adv Search |
DYNAMIC PROCESS OF MARTENSITIC STABILIZATION IN A Cu-Zn-Al ALLOY
by TAN Shusong; GAO Xiujuan (South-Central Polytechnic University) (Manuscript received 28 October; 1985; revised manuscript 18 July; 1986)
Cite this article: 

by TAN Shusong; GAO Xiujuan (South-Central Polytechnic University) (Manuscript received 28 October; 1985; revised manuscript 18 July; 1986). DYNAMIC PROCESS OF MARTENSITIC STABILIZATION IN A Cu-Zn-Al ALLOY. Acta Metall Sin, 1987, 23(6): 527-530.

Download:  PDF(349KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The dynamic process of stabilization of thermoelastic martensite in a Cu-Zn-Al alloy has been studied by means of electro-resistance and X-ray diffraction. It was found that the structure of the sample quenched into cold water (
Received:  18 June 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I6/527

1 谭树松,黄健超.中南矿冶学院学报,1984;(4) :19
2 祝向永,唐远永,曹明盛.中南矿冶学院学报,1981;(3) :1
3 Dunne D P, Kennon N F. Scr Metall, 1982; 16: 729
4 孔祥炎,高安娟.中南矿冶学院学报,1983;(2) :49
No related articles found!
No Suggested Reading articles found!