Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (6): 547-552    DOI:
Current Issue | Archive | Adv Search |
SOLUBILITY OF NIOBIUM CARBIDE IN A MICROALLOY STEEL
by ZHENG Lu; YONG Qilong; SUN Zhenbao (Central Iron and Steel Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 29 September; 1985; revised manuscript 8 April 1986)
Cite this article: 

by ZHENG Lu; YONG Qilong; SUN Zhenbao (Central Iron and Steel Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 29 September; 1985; revised manuscript 8 April 1986). SOLUBILITY OF NIOBIUM CARBIDE IN A MICROALLOY STEEL. Acta Metall Sin, 1987, 23(6): 547-552.

Download:  PDF(407KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The solubility of niobium carbide in γ-Fe of a microalloy steel, in which the Nb/C ratio is approximately equal to the stoichimetrie ratio of the carbide, has been determined by means of electrolytic extraction: lg([Nb]·[C]~(0.875))_v=2.97—7500/T±0.06(850—1200℃) The solubilities of it in γ-Fe and α-Fe have also been derived using the latest thermodynamic data, following results were obtained: lg([Nb]·[C]~(0.875))_v=3.24—7150/T(1100—1600K) lg([Nb]·[C]~(0.875))_0=4.87—10060/T(300—1000K)
Received:  18 June 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I6/547

1 Microalloying 75, Proc. of an Int. Symp. on High-Strength Low-Alloy Steel, New York; Union Carbide Corp., 1977
2 De Kazinczy F, Axans A, Pachleitner P. Jernkontorets Ann, 1963; 147: 408
3 小山伸二,石井辉雄,成田贵一.日本金属学会益,1971;35:698
4 盛利贞,时实正治,中嶋由行,佐伯俊秀。铁鋼,1965;51:2031
5 Irvine K J, Picketing F B, Gladman T. J Iron Steel Inst, London, 1967; 205: 161
6 Nordberg H, Aronsson B. J Iron Steel Inst, London, 1968; 206: 1263
7 Hudd R C, Jones A, Kale M N. J Iron Steel Inst, 1971; 209: 121
8 Narcta K. Trans Iron Steel Inst Jap, 1975; 15: 145
9 Lakshmanan V K, Kirkaldy J S. Metall Trans, 1984; 15A: 541
10 Sharma R C, Lakshmanan V K, Kirkaldy J S. Metall Trans, 1984; 15A: 545
11 雍岐龙,郑鲁.金属学报,1984;20:A9
12 雍岐龙,郑鲁,孙珍宝.金属学报,1986;22:A529
13 Chipman J. Metall Trans, 1972; 3: 55
14 Barin I, Dnacke O. Thermochemical Properties of Inorganic Substances, Berlin: Springer-Verlag. 1973, p, 116-118
15 Schenck H, Frohberg M G, Reinders F. Stahl Eisen, 1963; 83:93
16 Smith R P. Trans Metall Soc AIME, 1960; 224: 190
17 Hoogendoorn T M, Spanraft M J. Microailoying 75, Proc. of an Int. Symp, on High-Strength Low-Alloy Steel, New York: Union Carbide Corp., 1977, p. 7
No related articles found!