Abstract The activity of N in α-Fe was derived from the solubility data at580℃ in the Fe-N diagram. The interaction coefficients of Fe-N, Fe-C and C-Nwere obtained and the phase boundaries of single-phase ε-and γ_1-fields were subse-quently calculated. The results show that the γ_1-region of Naumann and LangescheidFe-C-N ternary phase diagram is correct, but the ε-region requires revision. Calcu-lation give an evidence that most of the experimental data on the ε-phase report-ed by Wells and Bell appears reasonable. Calculations taking graphite as a standaredstate confirms the above conclusions.
|
|
Received: 18 January 1988
|
1 Naumann F K, Langenscheid G A. Arch Eisenhuettenwesen, 1965; 36: 677 2 Raghavan V. Trans Indian Inst Met, 1984; 37(4) : 293 3 Wells A, Bell T. Heat Treat Met, 1983; 10: 39 4 Elliott J F, Gleiser M, Ramarkrishna V. In: Elliott J F, Gleiser M eds., Thermochemistry for Steelmaking, London: Addison-Wesley Publishing Co. Inc. 1963: 405 5 Darken L S, Gurry R W. Physical Chemistry of Metals, McGraw-Hill, 1953: 379 6 Reed T B. Free Energy of Formation of Binary Compounds, MIT Press, 1971: 26 7 Dew-Hughes D, Kaufman L. CALPHAD. 1979; 3: 175 8 冯端,王业宁,邱第荣.金属物理,上册,科学出版社,1964:69 9 Kaufman L.CALPHAD,1978;2:295 10 徐祖耀.金属材料热力学,科学出版社,1981:254 11 范鸣玉,张莹.最优化技术基础,清华大学出版社,1982:164B |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|