| KINETICS OF INTERACTION OF PbO, xPbO·SiO_2 WITH PbS AND ACTIVITY OF PbO |
| LIU Chunpeng Kunming College of Engineering LU Yuehua Post Graduate Student for Ph.D.;Department of Metallurgicel;Kunming Institute of Technology |
|
Cite this article:
LIU Chunpeng Kunming College of Engineering LU Yuehua Post Graduate Student for Ph.D.;Department of Metallurgicel;Kunming Institute of Technology. KINETICS OF INTERACTION OF PbO, xPbO·SiO_2 WITH PbS AND ACTIVITY OF PbO. Acta Metall Sin, 1988, 24(1): 119-122.
|
|
|
Abstract The rate equation for the reaction of PbO with PbS in liquidstate at 850--1000℃ has been determined as dα/dt=4.73×10~6 exp (-190/RT)in which the activation en ergy E=190kJ/mol. In the solid-liquid reaction system of xPbO. SiO_2-PbS, the rate equation maybe formulated as following: dF(α)/dt=k′(t<20min)+k"(t>20min) (1000℃)where F(α)=α-(N°_(SiO_2/N°_(PbO))ln(1-α) The activities of PbO and SiO_2 in the silicate calculated from the rate dataare in good agreement with those measured thermodynamically.
|
|
Received: 18 January 1988
|
1 #12 2 Shohu H Y,Wodsworth M E.郑蒂基译. 提取冶金速过程,北京:冶金工业出版社,1984:153 3 李振家,芦爱春,孙萼庭.全国第一届冶金过程物理化学学术论文集,上海科学技术出版社,1962:380 4 Liou Chunpen, Feng Ganming, Yan Chuanyi, Ho Aiping, First China-USA Bilateral Mctallurgical Conference, Beijing, 1981: 137 5 Richardson F D. WebbL E. Bull Inst Met. 1955; 64: 529 6 Kozuka Z, Samis C S. Met Trans, 1970; 1: 8717 |
| No Suggested Reading articles found! |
|
|