Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (1): 1-6    DOI:
Current Issue | Archive | Adv Search |
OBSERVATION OF EPITAXIAL OVERLAYER OF METALS AT ATOMIC LEVEL
GAO Qiaojun;T. T. TSONG Beijing University Pennsylvania State University U. S. A
Cite this article: 

GAO Qiaojun;T. T. TSONG Beijing University Pennsylvania State University U. S. A. OBSERVATION OF EPITAXIAL OVERLAYER OF METALS AT ATOMIC LEVEL. Acta Metall Sin, 1989, 25(1): 1-6.

Download:  PDF(1549KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Observation of epitaxial overlayer of metals at atomic level has beensuccessfully observed in field ion microscope with 5 ns pulsed-laser heating. Thecondition of superlattice layer growth depends on the surface free energy and thelattice misfit. Many defects, such as vacancies, vacancy clusters, voids, dislocationsand twins are produced during epitaxial growth because of the lattice misfit eventhough the condition of surface free energy is satisfied. Alloying is observed tooccur on the surface of the metal during the epitaxial growth. Diffusion is proba-bly via the exchange mechanism.
Key words:  Field ion microscope      epitaxial growth      crystal defect      diffusion mechanism      superlattice     
Received:  18 January 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I1/1

1 Graham W R, Hutchinson F, Nadakavukaren J J, et. al. J Appl Phys, 1969; 40: 3931
2 Tsong T T, Casanova R. Phys Rev Lett, 1981; 47: 113
3 Fink H W, Ehrlich G. Surf Sci, 1981; 110: L611
4 Bruce L A, Jaeger H. Philos Mag, 1978; A38: 223
5 Tsong T T. Prog Surf Sci, 1980; 10: 165
6 Bauer E, Van der Merwe Jan H. Phys Rev, 1986; B33: 3657
7 Gao Q J (高巧君), Tsong T T (郑天佐). Phys Rev Lett, 1986; 57: 452
8 Tsong T T, Gao Q J. Phys Rev, 1987; B35: 7764
9 Gao Q J, Tsong T T. Phys Rev, 1987; B36: 2547
10 Ramirez R, Rahman A, Schuller Ivan K. Phys Rev, 1984; B30: 6208
11 Matthews J W, Jesser W A. Acta Metall, 1967; 15: 595
[1] SUN Zhengyang, YANG Chao, LIU Wenbo. Phase Field Simulations of the Sintering Process of UO2[J]. 金属学报, 2020, 56(9): 1295-1303.
[2] YANG Gaolin, LIN Xin, HU Qiao, ZHANG Ying, WANG Zhitai, LI Peng, HUANG Weidong. CRYSTALLIZATION BEHAVIOR OF ANNEALED Zr55Cu30Al10Ni5 BULK METALLIC GLASS  DURING PULSED LASER REMELTING[J]. 金属学报, 2013, 49(6): 649-657.
[3] Bilong Li; Geyang Li. Microstructures and Mechanical Properties of TiN/AlON Nanomultilayers synthesized by Reactive Magnetron Sputtering[J]. 金属学报, 2008, 44(2): 193-197 .
[4] Ge-Yang LI. Study on the Sensitivity of Mechanical Properties of TiN/Si3N4 Nano-structured Film to Si3N4 Layer Thickness[J]. 金属学报, 2007, 43(2): 154-158 .
[5] ZHONG Minlin;LIU Wenjin;YAO Kefu;REN Jialie;HU Shuqiang;ZHAO Hong (Tsinghua Universtty; Beijing 100084)(Manuscript received 1996-06-10; in revised form 1996-08-12). CW LASER GLAZING OF Fe-C-Si-B ALLOY AND FORMING CONDITION OF METALLIC GLASSES[J]. 金属学报, 1997, 33(4): 413-419.
[6] RONG Yonghua;WU Hiaohua;CHEN Hiaofu;CHEN Shipu;HU Gengxiang;(Shanghai Jiaotong University;Shanghai 200030)(Manuscript received l994-06-l6;in revised form 1994-12-04). TEM AND COMPUTER IMAGE SIMULATIONS ON SUPERDISLOCATIONS IN ROOM TEMPERATURE DEFORMED Al_(67)Mn_8Ti_(25) ALLOY[J]. 金属学报, 1995, 31(7): 294-299.
[7] ZHAO Xingzhong; WU Xingfang; KE Jun (University of Science and Technology Beijing)(Manuscript received 18 June; 1993; in revised form 29 November; 1993). METASTABLE x-PHASE IN TiNi SHAPE MEMORY ALLOY[J]. 金属学报, 1994, 30(7): 302-306.
[8] YU Zongsen;CHEN Ning(University of Science and Technology Beijing)(Manuscript received 21 June;1993). A NEWLY DISCOVERED DIFFUSION MECHANISM IN SOLIDS──COMPLEX DIFFUSION MECHANISM[J]. 金属学报, 1994, 30(1): 7-10.
[9] LI Fengzhao;DAI Jiyan;LI Douxing Shandong Polytechnic University; Jinan; Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Academia Sinica; Shenyang Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Academia Sinica; ShenyangSUN Dongsheng;assoeiate professor.Institute of Materials Engineering.Shandong Polytechnic University ;Jinan 250014. CRYSTAL DEFECTS AND INTERFACE STRUCTURE OF ION-NITRIDED LAYERS[J]. 金属学报, 1993, 29(5): 11-15.
[10] WANG Bosheng;SUN Fuyu;MENG Qing'en;XU Wenchong Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. AN APPROACH TO MATHEMATICAL MODELING OF DISLOCATION LINK LENGTH DISTRIBUTION IN METAL[J]. 金属学报, 1992, 28(3): 6-9.
[11] SUN Yangshan;GUO Jun;ZHANG Lining;ZHANG Jinping Southeast University; Nanjing. EFFECTS OF Ce AND Cr ON ROOM TEMPERATURE MECHANICAL PROPERTIES OF Fe_3 Al[J]. 金属学报, 1991, 27(4): 11-16.
[12] BI Siyun;MA Xiaoding;SONG Ruitian;MEI Liangmo;ZHAO Jiangao;GUO Yicheng Shandong University; Jinan. STRUCTURE AND FERROMAGNETIC RESONANCE OF METAL Fe/Cu SUPERLATTICES[J]. 金属学报, 1990, 26(5): 131-136.
[13] LIU Zhiguo;CHEN Yong;CAO Yanni;ZHU Zhengsheng Nanjing University Shanxi Iron and Steel Institute; Xi'an professor;Department of Physics;Nanjing University;Nanjing 210008. PRECIPITATION HARDENING OF ELINVAR ALLOY[J]. 金属学报, 1990, 26(4): 40-44.
[14] ZHU Min;YANG Dazhi Dalian University of Technology. A NEW KIND OF QUENCHING INDUCED PLANAR DEFECT OF MARTENSITE IN Cu-Zn-Al ALLOY[J]. 金属学报, 1989, 25(2): 74-76.
No Suggested Reading articles found!