Acta Metall Sin  1989, Vol. 25 Issue (3): 90-95    DOI:
Current Issue | Archive | Adv Search |
CALCULATION OF NaCl-BaCl_2-SrCl_2 PHASE DIAGRAM
LI Ruiqing;ZHOU Guozhi Beijing General Research Institute for Non-Ferrous Metals University of Science and Technology Beijing
Cite this article: 

LI Ruiqing;ZHOU Guozhi Beijing General Research Institute for Non-Ferrous Metals University of Science and Technology Beijing. CALCULATION OF NaCl-BaCl_2-SrCl_2 PHASE DIAGRAM. Acta Metall Sin, 1989, 25(3): 90-95.

Download:  PDF(403KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The mathematical formulas are given for calculating the partial molarthermodynamic properties in a ternary system from its three corresponding binary sys-tems based on the new ternary symmetric model presented by the authors in theforegoing paper. Applying this model to NaCl-BaCl_2-SrCl_2 system, the phase diagramof which as well as some isothermal sections have been calculated. The deviations oftemperature between the calculated and experimental diagrams are less than five de-grees.
Key words:  symmetric geometry model      ternary phase diagram of molten salts     
Received:  18 March 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I3/90

1 Levin E M, Robbins C R, Mcmurdie H F. In: Reser M K ed, Phase Diagrams for Ceramists. and 1969, 1975 Suppl., Columbus, Ohio: American Ceramic Society, Fig. 1428
2 周国治,李瑞青.稀有金属,待发表
3 Barin I, Knacke O, Kubaschewski O. Thermochemical Properties of Inorganic Substances, Springer-Verlag, Berlin, 1977
4 Levin E M, Robbins C R, Mcmurdie H F. In: Reser M K ed, Phase Diagrams for Ceramists, and 1969, 1975 Suppl., Columbus, Ohio: American Ceramic Society, Fig. 1311
5 Emons H H, Brautigan G, Thomas R. Chem Zvesti, 1978; 32 (6) : 721
6 1968; 13 (8) ; 2251
7 Levin E M, Robbins C R, Mcmurdie H F. In: Reser M K ed, Phase Diagrams for Ceramists, and 1969, 1975 Suppl., Columbus. Ohio: American Ceramic Society, Fig. 1301
8 Egan J J. Bracker J. J Chem Thermodyn, 1974; 6: 9
9 Qiao Zhiyu (乔芝郁), James Sangster. Pelton A D. CALPHAD, 1987; 11:
10 Papatheodorou G N. Kleppa O J. J Chem Phys, 1967; 47: 2014
No related articles found!
No Suggested Reading articles found!