EFFECT OF OXYGEN CONTENTS ON OXYGEN POTENTIALS OF H_2O-H_2 AND H_2O-H_2-INERTS GAS MIXTURES
FANG Zheng;CHEN Xinmin H. M Chen Central South University of Technology; Changsha
Cite this article: 

FANG Zheng;CHEN Xinmin H. M Chen Central South University of Technology; Changsha. EFFECT OF OXYGEN CONTENTS ON OXYGEN POTENTIALS OF H_2O-H_2 AND H_2O-H_2-INERTS GAS MIXTURES. Acta Metall Sin, 1989, 25(4): 81-88.

Download:  PDF(624KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By taking the effect of oxygen contents into account, a new set offormulae which represents the oxygen potentials of H_2O-H_2 and H_2O-H_2-inerts gasmixtures has been derived. Classical representation is only a particular case of it.Some of the variables affecting the equilibrium atmosphere when trace oxygen ispresent and optimum preparation of the gas mixtures to minimize errors have beendiscussed. The reliability of some of previous equilibrium experiments under theoxygen potentials controlled by H_2O-H_2 or H_2O-H_2-inerts gas mixtures has alsobeen criticized.
Key words:  gas equilibration method      H_2O-H_2      H_2O-H_2-inerts      oxygen potential     
Received:  18 April 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I4/81

1 Emmett P H, Shultz J F. J Am Chem Soc, 1929; 51: 3249
2 Shibata Z, Kitagawa H. J Fac Sci, 1938; 2: 223
3 Muan A. Am J Sci, 1958; 256 (3) : 171
4 Pierre G R St., Ebihara W T, Pool M J, Speiser R. Trans AIME, 1962; 224: 259
5 Rapp R A. Physicochemical Measurements in Metals Research, Vol. Ⅳ, New York: Interscience, 1970: 338
6 Gaskell D R. Introduction to Metallurgical Thermodynamics. 2nd Ed., New York: Hemisphere Publishing, 1981: 242
7 王常珍.冶金物理化学研究方法,北京:冶金工业出版社,1982:230
8 方正,陈新民.中南矿冶学院学报,1982;13(4) :1
9 方正,陈新民.金属学报,1988;24:B41
10 方正,陈新民.第七届冶金过程物理化学年会和第二届有色冶金物理化学年会论文集,中国金属学会,中国有色金属学会,沈阳,1989:59
11 Sardi A. Acta Chim Hung, 1963; 38: 177
[1] FANG Zheng;CHEN Xinmin (H. M. Chen) Central South University of Technology; ChangshaFANG Zheng;Dr.and Lecture;Department of Chemistry Cental-South Universisy of Thechnology;Changsha. EQUILIBRIUM BETWEEN NONSTOICHIOMETRIC Mo AND MoO_2——WITH APPLICATION OF SIEVERTS' LAW CONSTANT TO SMILTENS' INTEGRATION[J]. 金属学报, 1988, 24(1): 111-113.
No Suggested Reading articles found!