Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (6): 131-135    DOI:
Current Issue | Archive | Adv Search |
QUANTITATIVE RELATION BETWEEN YIELD STRESS AND R-VALUE ALONG DIRECTIONS PARALLEL AND PERPENDICULAR TO ROLLED Ti PLATE
ZHANG Derong Shenyang Institute of Aeronautical Engineering ZHANG Derong; associate professor; Department of Aeronautics; Shenyang Institute of Aeronautical Engineering; Shenyang 110031
Cite this article: 

ZHANG Derong Shenyang Institute of Aeronautical Engineering ZHANG Derong; associate professor; Department of Aeronautics; Shenyang Institute of Aeronautical Engineering; Shenyang 110031. QUANTITATIVE RELATION BETWEEN YIELD STRESS AND R-VALUE ALONG DIRECTIONS PARALLEL AND PERPENDICULAR TO ROLLED Ti PLATE. Acta Metall Sin, 1989, 25(6): 131-135.

Download:  PDF(353KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An attempt was made on the quantitative prediction of the relation-ship batween yield stress and R-value along the directions parallel and perpendicul-ar to rolled Ti plate based on analysis of the previous experimental data. It is sh-own that the yield stress along one direction and another is synchronized withR-value. Based on the theory of plasticity a formula of σ_(1s)/σ_(7s)=[1+1/R_2)/(1+1/R_1)]~(1/2)was proposed. In statistic estimation, the calculated results after the formula are inbetter agreement with the experimental data. The availability of this formula wasbriefly discussed also.
Key words:  Ti plate      yield stress      R-value     
Received:  18 June 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I6/131

1 周维贤.TC1钛板的机械性能及其异性情况,西北工业大学科技资料,总字第1059期,1979
2 翟平.TA2M钛板机械性能及各向异性,西北工业大学科技资料,ZHZ8018,1981
3 周维贤.剖面收缩率在评估钛板成形性方面的意义,中国航空学会飞机制造技术学术交流会资料,1988
4 Hill R. The Mathematical Theory of Plasticity. Oxford at the Clarendon Press, 1950: 317--340
5 Slater R A C.王仲仁,袁祖培译.工程塑性理论及其在金属成形中的应用,机械工业出版社’1983:141
6 王仁,熊祝华,黄文彬.塑性力学基础,科学出版社,1982:176
7 Babel H W, Eitman D A, McIver R W. ASM Trans D: J Basic Eng, 1967; 89(1) : 13
8 张德荣.沈阳航空工业学院学报,1987;(1) :29
[1] ZHU Wenhui; ZHOU Guangquan; CHENG Jingyi(University Scicnce Technology; Hefei 230026)(National University Defence Technology; Changsha 410073). DEPENDENCE OF YIELD STRESS ON GRAIN SIZE OF NANOCRYSTALS[J]. 金属学报, 1996, 32(9): 959-965.
[2] LUO Jingxi; TONG Mingxin(State Key Laboratory for Mechanical Behaviour of Materials; Xi'an Jiaotong University; Xi'an 710049)(Manuscript received 1995-10-20; in revised form 1996-02-02). EFFECTS OF COTTRELL ATMOSPHERE ON INITIAL YIELD STRESS AND FATIGUE THRESHOLD OF STEEL 20CrMO[J]. 金属学报, 1996, 32(8): 834-838.
[3] GAI Hiuying; LI Jiabao; KANG Zengqiao; WANG Zhongguang (State Key Laboratory for Fatigue and Fracture of Materials;Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)ZHU Yongping; LI Chao (Shenyang Polytechnical University; Shenyang 110023). MECHANICAL PROPERTIES OF SHOT PEENED SURFACE FOR STEEL 60Mn[J]. 金属学报, 1996, 32(6): 605-610.
[4] TANG Changguo (Northwestern Polytechnical University; Xi'an 710072)ZHU Jinhua;ZHOU Huijiu (State Laboratory for Mechanical Behaviour of Materials;Xi'an Jiaotong University 710049). CORRELATION BETWEEN YIELD STRESS AND STRAIN RATE FOR METALLIC MATERIALS AND THERMAL ACTIVATION APPROACH[J]. 金属学报, 1995, 31(6): 248-253.
[5] ZHOU Weixian Northwestern Polytechnical University; Xi'an. QUANTITATIVE RELATIONSHIP BETWEENYIELD STRESS AND r-VALUE OF Ti SHEET[J]. 金属学报, 1991, 27(6): 44-49.
No Suggested Reading articles found!