| TRANSFER OF Ti AND Si BETWEEN SLAGS AND MOLTEN Cu UNDER CONSTANT OXYGEN POTENTIAL |
| XUE Xiangxin;DU Hegui Northeast University of Technology; Shenyang Department of Ferrous Metallurgy;Northeast University of Technology; Shenyang 110006 |
|
Cite this article:
XUE Xiangxin;DU Hegui Northeast University of Technology; Shenyang Department of Ferrous Metallurgy;Northeast University of Technology; Shenyang 110006. TRANSFER OF Ti AND Si BETWEEN SLAGS AND MOLTEN Cu UNDER CONSTANT OXYGEN POTENTIAL. Acta Metall Sin, 1990, 26(2): 146-148.
|
|
|
Abstract An experimental study has been made of the mass transfer of Ti and Si betweenslags and molten Cu under constant oxygen potential at 1500℃. Apparent mass transfer coeffi-cients of Ti and Si in molten Cu were obtained.
|
|
Received: 18 February 1990
|
1 Baxter G P, Lansing J E. J Amer Chem Soc, 1920; 42: 419 2 周继程,邹元爔,赵彭年,李鸿明,张子青.中国金属学会编,中国金属学会1979--1980年优秀论文集,第四分册,北京:冶金工业出版社,1984:83 3 森一美,平沢政(广厶),新贝元,圃中朝夫.铁钢,1985;71:1110 4 薛向欣,杜鹤桂.金属学报,1990;26:B7 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|