SOLUTION BEHAVIOUR OF VARIOUS ALLOYING ELEMENTS IN Ni_3 Si
LI Yundong;ZHANG Tianxiang;ZHENG Zhi;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang professor;Institute of Metal Reseacrh;Academia Sinica Shenyang 110015
Cite this article: 

LI Yundong;ZHANG Tianxiang;ZHENG Zhi;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang professor;Institute of Metal Reseacrh;Academia Sinica Shenyang 110015. SOLUTION BEHAVIOUR OF VARIOUS ALLOYING ELEMENTS IN Ni_3 Si. Acta Metall Sin, 1990, 26(3): 18-22.

Download:  PDF(440KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The solid solubilities of 15 common alloying elements added to theLl_2-type intermetallic compound Ni_3Si at 900℃ have been estimated, and their sub-stitution modes have been deduced from the direction of solubility lobe of the com-pound. It is shown that the alloying behaviours in Ni_3Si are determined by bothsize and electronic factors, i. e., the substitution behaviour by electronic configura-tion and solubility by the both. An interaction parameter is presented to describequantitatively the influence of electronic configuration on substitution behaviour andthe solubility limit can be successfully explained together with atom radii.
Key words:  alloying behaviour      atom size      electronic configuration      interaction parameter     
Received:  18 March 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I3/18

1 Mishima Y, Oya Y, Suzuki T. Trans, Iron Steel Inst Jpn, 1985; 25: 1171
2 Meier G H. In: Koch C C, Liu C T, Stoloff N S, Izumi O eds., High Tamperature Ordered Intermetallic Alloys II, Pittsburgh: Materials Research Society, 1987: 443
3 Evans T E, Hart A C. Electrochim Acta, 1971; 16: 1955
4 Takasugi T, Izumi O. Acta Metall, 1985; 33: 1247
S Liu C T. In: Koch C C, Liu C T, Stoloff N S, Izumi O eds., High Temperature Ordered Intermetallic Alloys II, Pittsburgh: Waterials Research Society, 1987: 355
6 Oya Y, Ochiai S, Shinoda T Suzuki T. Z Metallk. 1984; 75: 53
7 Takasugi T, Izumi O, Masahashi N. Acta Metall, 1985; 33: 1259
8 Ochiai S, Oya Y, Suzuki T. Acta Metall. 1984; 32: 289
9 虞觉奇,易文质,陈帮迪,陈宏鉴,二元合金状态图集,上海科学技术出版社,1987:704I
[1] ZHANG Lili, JI Zongwei, ZHAO Jiuzhou, HE Jie, JIANG Hongxiang. Key Factors Influencing Eutectic Si Modification in Al-Si Hypoeutectic Alloy by Trace La[J]. 金属学报, 2023, 59(11): 1541-1546.
[2] . Quasicrystals in Al-Cu-Ni-Fe Quaternary System[J]. 金属学报, 2007, 43(4): 374-378 .
[3] LUO Lihua; DING Xueyong; GUO Dan; CAO Wenbin; ZOU Zongshu; WANG Wenzhong (School of Materials and Metallurgy; Northeastern University; Shenyang 110006)( University of Science and Technology Beijing; Beijing 1100083). DATABASE SOFTWARE DEVELOPMENT FOR ACTIVITY AND INTERACTION MRAMETER OF ALLOY SYSTEMS[J]. 金属学报, 1998, 34(4): 388-392.
[4] G Xueyong(Northeastern University;Shenyang);FAN Peng;HAN Qiyong(University of Science and Technology Beijing)(Manuscript received 8 April;1993;in revised form 15 July;1993). MODELS OF ACTIVITY AND ACTIVITY INTERACTION PARAMETER IN TERNARY METALLIC MELT[J]. 金属学报, 1994, 30(14): 49-60.
[5] DING Xueyong;WANG Wenzhong;HAN Qiyong Northeastern University University of Science and Technology Beijing. THERMODYNAMIC CALCULATION OF Fe-P-j SYSTEM MELT[J]. 金属学报, 1993, 29(12): 21-26.
[6] LIU Huanming;YANG Zupan;TIAN Yanwen The Steel Works No.2; Benxi Iron and Steel Company Northeast University of Technology; Shenyang LIU Huanming; assistant engineer; the Laboratory of Steel Works No.2; Benxi Iron and Steel Company; Benxi; Ltaoning. SELF-REACTION COEFFICIENTS OF Ca AND Mg IN LIQUID Sn[J]. 金属学报, 1989, 25(5): 79-84.
No Suggested Reading articles found!