| SOLUTION BEHAVIOUR OF VARIOUS ALLOYING ELEMENTS IN Ni_3 Si |
| LI Yundong;ZHANG Tianxiang;ZHENG Zhi;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang professor;Institute of Metal Reseacrh;Academia Sinica Shenyang 110015 |
|
Cite this article:
LI Yundong;ZHANG Tianxiang;ZHENG Zhi;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang professor;Institute of Metal Reseacrh;Academia Sinica Shenyang 110015. SOLUTION BEHAVIOUR OF VARIOUS ALLOYING ELEMENTS IN Ni_3 Si. Acta Metall Sin, 1990, 26(3): 18-22.
|
|
|
Abstract The solid solubilities of 15 common alloying elements added to theLl_2-type intermetallic compound Ni_3Si at 900℃ have been estimated, and their sub-stitution modes have been deduced from the direction of solubility lobe of the com-pound. It is shown that the alloying behaviours in Ni_3Si are determined by bothsize and electronic factors, i. e., the substitution behaviour by electronic configura-tion and solubility by the both. An interaction parameter is presented to describequantitatively the influence of electronic configuration on substitution behaviour andthe solubility limit can be successfully explained together with atom radii.
|
|
Received: 18 March 1990
|
1 Mishima Y, Oya Y, Suzuki T. Trans, Iron Steel Inst Jpn, 1985; 25: 1171 2 Meier G H. In: Koch C C, Liu C T, Stoloff N S, Izumi O eds., High Tamperature Ordered Intermetallic Alloys II, Pittsburgh: Materials Research Society, 1987: 443 3 Evans T E, Hart A C. Electrochim Acta, 1971; 16: 1955 4 Takasugi T, Izumi O. Acta Metall, 1985; 33: 1247 S Liu C T. In: Koch C C, Liu C T, Stoloff N S, Izumi O eds., High Temperature Ordered Intermetallic Alloys II, Pittsburgh: Waterials Research Society, 1987: 355 6 Oya Y, Ochiai S, Shinoda T Suzuki T. Z Metallk. 1984; 75: 53 7 Takasugi T, Izumi O, Masahashi N. Acta Metall, 1985; 33: 1259 8 Ochiai S, Oya Y, Suzuki T. Acta Metall. 1984; 32: 289 9 虞觉奇,易文质,陈帮迪,陈宏鉴,二元合金状态图集,上海科学技术出版社,1987:704I |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|