Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (4): 40-44    DOI:
Current Issue | Archive | Adv Search |
PRECIPITATION HARDENING OF ELINVAR ALLOY
LIU Zhiguo;CHEN Yong;CAO Yanni;ZHU Zhengsheng Nanjing University Shanxi Iron and Steel Institute; Xi'an professor;Department of Physics;Nanjing University;Nanjing 210008
Cite this article: 

LIU Zhiguo;CHEN Yong;CAO Yanni;ZHU Zhengsheng Nanjing University Shanxi Iron and Steel Institute; Xi'an professor;Department of Physics;Nanjing University;Nanjing 210008. PRECIPITATION HARDENING OF ELINVAR ALLOY. Acta Metall Sin, 1990, 26(4): 40-44.

Download:  PDF(601KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructural evolution and precipitation hardening of an Elin-var alloy doped with Ti and Al during isothermal aging at 700℃ have been inves-tigated by atom probe field ion microscopy and microhardness measurement. Theγ′ precipitates formed are spherical and coherent with the matrix. The chemical com-position of the precipitates are (Ni_(0.53)Fe_(0.47))_3(Ti_(0.6)Al_(0.4)). During aging, a Lifshitz-Wanger type dissolution and coarsening reaction of the precipitates has been obse-rved. The hardness of the material varies with the aging time and reaches maxi-mum when the average diameter of the precipitates was about 11 nm.
Key words:  Elinvar alloy      atom probe field ion microscope      γ′phase precipitation      precipitation hardening      atom probe selected area analysis     
Received:  18 April 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I4/40

1 Chen Y, Liu Z G, Cao Y N, Zhu Z S. Scr Metall, 1988; 22: 1075
2 Liu Z G, Chen Y, Feng D. Z Metallkde, 1988; 79: 643
3 Miller M K. Int Metall Rev, 1987; 32: 221
4 Lifshitz I M, Slyozov V V, J Phys Chem Solids, 1961; 19; 35
5 Wagner C. Z Elektrochem, 1961; 65: 581
[1] Qin SHEN,Xiaojiao WANG,Anyu ZHAO,Yifeng HE,Xulei FANG,Jiarong MA,Wenqing LIU. EFFECTS OF Mn ON MULTI-PRECIPITATES EVOLUTION OF Cu-RICH AND NiAl PHASE IN STEELS[J]. 金属学报, 2016, 52(5): 513-518.
[2] Ke ZHANG,Qilong YONG,Xinjun SUN,Zhaodong LI,Peilin ZHAO. EFFECT OF COILING TEMPERATURE ON MICRO-STRUCTURE AND MECHANICAL PROPERTIES OF Ti-V-Mo COMPLEX MICROALLOYED ULTRA-HIGH STRENGTH STEEL[J]. 金属学报, 2016, 52(5): 529-537.
[3] CHEN Jun, TANG Shuai, LIU Zhenyu, WANG Guodong. EFFECTS OF COOLING PROCESS ON MICROSTRUCTURE, MECHANICAL PROPERTIES AND PRECIPITATION BEHAVIORS OF NIOBIUM-TITANIUM MICRO-ALLOYED STEEL[J]. 金属学报, 2012, 48(4): 441-449.
[4] WANG Qing ZHA Qianfeng LIU Enxue DONG Chuang WANG Xuejun TAN Chaoxin JI Chunjun. COMPOSITION DESIGN OF HIGH–STRENGTH MARTENSITIC PRECIPITATION HARDENING STAINLESS STEELS BASED ON A CLUSTER MODEL[J]. 金属学报, 2012, 48(10): 1201-1206.