FORMATION OF AMORPHOUS Al_(80)Fe_(20) BY MECHANICAL ALLOYING
WANG Weihua;XIAO Keqin;CHU Zhaoqin;DONG Yuanda;WANG Gengmiao Institute of Solid State Physics; Academia Sinica; Hefei Centre of Structural Analysis; China University of Science and Technology; Hefei
Cite this article: 

WANG Weihua;XIAO Keqin;CHU Zhaoqin;DONG Yuanda;WANG Gengmiao Institute of Solid State Physics; Academia Sinica; Hefei Centre of Structural Analysis; China University of Science and Technology; Hefei. FORMATION OF AMORPHOUS Al_(80)Fe_(20) BY MECHANICAL ALLOYING. Acta Metall Sin, 1990, 26(5): 97-101.

Download:  PDF(449KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The mechanical alloying was successfully utilized to make an amor-phous Al_80Fe_20 powder from pure crystalline Fe and Al powders, but no other con-ventional rapid solidification process to be formed. The amorphization process wasexamined by X-ray analysis and Mossbauer spectroscopy, and the thermal behavi-our was studied by DSC. The results show that the rate of amorphization is con-trolled by the diffusion reaction at the interfaces and changes with the milling time.The effect of milling conditions on amorphization by mechanical alloying was alsoinvestigated.
Key words:  mechanical alloying      amorphization      Al-Fe amorphous alloy      Mossbauer spectrum analysis     
Received:  18 May 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I5/97

1 Johnson W L. Prog Mater Sci, 1986; 30: 81
2 Samwer K. Phys Rep, 1988; 16: 1
3 Koch C C, Cavin O B, McKamey C G, Scarbrough J O. Appl Phys Lett, 1983; 43: 1017
4 Schultz L. Mater Sci Eng, 1988; 97: 15
5 Weeber A W, Bakker H. Physica, B+C, 1988; 153: 93
6 Matsuki K, Inoue A, Kimura H M, Masumoto T. Mater Sci Eng, 1988; 97: 47
7 Perz Alcazar G A, da Silva E G. J Phys F: Met Phys, 1987; 17: 2323
8 Dong Yuanda. to be published
9 Schurer P J, Koopmans B, van der Woude F, Bronsveld P. Solid State Commun, 1986; 59: 619
10 Rao V S, Mani B. International Conference on the Applications of the Mossbauer Effect, India, 1981, New Delhi: Indian National Science Academy, 1981: 474
11 Aharoni A. Phys Rev, 1973; B7: 1103
[1] Min ZHU, Zhongchen LU, Renzong HU, Liuzhang OUYANG. DIELECTRIC BARRIER DISCHARGE PLASMA ASSISTED BALL MILLING TECHNOLOGY AND ITS APPLICATIONS IN MATERIALS FABRICATION[J]. 金属学报, 2016, 52(10): 1239-1248.
[2] HU Na, XUE Lihong, GU Jian, LI Heping, YAN Youwei. OPTIMIZATION OF GRADING ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Al13Fe4/Al COM- POSITES IN SITU SYNTHESIZED BY MECHANICAL ALLOYING AND SPARK PLASMA SINTERING[J]. 金属学报, 2015, 51(2): 216-222.
[3] GU Jian, GU Sasa, XUE Lihong, WU Shusen, YAN Youwei. MICROSTRUCTURE EVOLUTION OF Al-Fe ALLOYS PREPARED BY MECHANICAL ALLOYING AND SPARK PLASMA SINTERING[J]. 金属学报, 2013, 29(4): 435-442.
[4] WANG Man, ZHOU Zhangjian, YAN Zhigang, YU Pengfei, SUN Hongying. TEM CHARACTERIZATION OF DISPERSOIDS AND MICROSTRUCTURE OF ODS-316 AUSTENITIC STEEL[J]. 金属学报, 2013, 49(2): 153-158.
[5] LU Zheng, LU Chenyang, ZHANG Shouhui, XIE Rui, Liu Chunming. PREPARATION AND CHARACTERIZATION OF NANO-STRUCTURED 14Cr-ODS FERRITIC STEEL[J]. 金属学报, 2012, 48(6): 649-653.
[6] ZHANG Laichang; SHEN Zhiqi; XU Jian. The Role of Sn Substitution for Si And B to Enhance the Amorphization of Mechanically-Milled Ti50Ni22Cu18Al4Si4B2 Alloy[J]. 金属学报, 2004, 40(9): 981-986 .
[7] ZHANG Xiaoqiang; XU Jian. Formation of W Particles /La55Al25Cu10Ni5Co5 Glassy Alloy Matrix Composites By Mechanical Milling[J]. 金属学报, 2004, 40(6): 647-.
[8] HANG Laichang; SHEN Zhiqi; XU Jian. MECHANICALLY--DRIVEN AMORPHIZATION IN A (Ti, Zr, Hf)--(Cu, Ni, Ag)--Al MULTICOMPONENT ALLOY SYSTEM[J]. 金属学报, 2004, 40(4): 421-428 .
[9] REN Shan; HONG Lan; ZHANG Jinxiu (Department of Physics; Zhongshan University; Guangzhou 510275)LU Manqi; HU Zhuangqi (State Key Lab of RSA; Institute of Metal Research; Shenyang 110015). HYDROGEN INDUCING AMORPHIZATION OF Ti-Fe SYSTEM IN MECHANICAL ALLOYING[J]. 金属学报, 1998, 34(4): 373-377.
[10] TIAN Yun;PAN Qingchun;LIU Guangzu;SHAN Bingquan;YANG Fenglan (Central Iron and Steel Research Institute; Beijing 100081). EFFECTS OF Ti ON STRENGTHENING OF ODS FERRITIC ALLOY FOR ADVANCED FBR CLADDING APPLICATION[J]. 金属学报, 1998, 34(11): 1217-1222.
[11] YANG Junyou; WU Jiansheng; ZENG Zhenpeng(The Open Laboratory of Education Ministry for High Temperature Materials and High Temperature Tests;Shanghai Jiaotong University; Shanghai 200030)Correspondent: YANG Junyou; postdoctoral research;Tel: (021)62812440;E-mail: jggang@ mail.sjtu.edu.cn. INVESTIGATION ON THE DEFORMATION AND ENERGY TRANSFER OF POWDERS DURING MECHANICAL ALLOVING[J]. 金属学报, 1998, 34(10): 1061-1067.
[12] MEI Zhi;GU Mingyuan;WU Renjie (State Key Laboratory of Metal Matrix Composites; Shanghai Jiaotong University;Shanghai 200030). AMORPHIZATION OF SURFACE OXIDIZED LAYER OF SiC IN SiC_p/AlCOMPOSITE[J]. 金属学报, 1997, 33(5): 557-560.
[13] LI Bolin;ZHU Min; LI Long; LUO Kanchang;LI Zuxin (South China University of Technology; Guangzhou 510641)(Manuscript received 1996-03-19; in revised form 1996-07-15). HARDENNING AND SOFTENNING EFFECTS OF Fe-Cu NANOCRYSTALLINE SUPERSATURATED SOLID SOLUTION FORMED BY MECHANICAL ALLOYING[J]. 金属学报, 1997, 33(4): 420-426.
[14] YANG Junyou; ZHANG Tongjun; CUI Kun; HU Zhenhua (Huazhong University of Science and Technology; Wuhan 430074)(Manuscript received 1996-03-18). ANALYSIS OF IMPACT BEHAVIOR DURING BALL MILLING[J]. 金属学报, 1997, 33(4): 381-385.
[15] ZHOU Lanzhang;GUO Jianting;QUAN Mingxiu(Institute of Metal Research;The Chinese Academy of Sciences;Shenyang 110015). FORMATION MECHANISM OF NiAl/TiC NANOCOMPOSITE BY MECHANICAL ALLOYING[J]. 金属学报, 1997, 33(11): 1222-1226.
No Suggested Reading articles found!