Acta Metall Sin  1992, Vol. 28 Issue (5): 21-25    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF La ON SNOEK-KE-K■STER PEAK IN Fe-P-N ALLOY
JI Jingwen;WEI Quanjin;ZHANG Guofu;LAI Zuhan;CHEN Tingguo Northeast University of Technology; Shenyang; Shanghai Institute of Metallurgy; Academia Sinica; Correspondent associate professor; Department of physics; Northeast University of Technology; Shenyang 110006)
Cite this article: 

JI Jingwen;WEI Quanjin;ZHANG Guofu;LAI Zuhan;CHEN Tingguo Northeast University of Technology; Shenyang; Shanghai Institute of Metallurgy; Academia Sinica; Correspondent associate professor; Department of physics; Northeast University of Technology; Shenyang 110006). EFFECT OF La ON SNOEK-KE-K■STER PEAK IN Fe-P-N ALLOY. Acta Metall Sin, 1992, 28(5): 21-25.

Download:  PDF(406KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Effect of various contents of La additive in Fe-P-N alloy on theirSnoek-Ke-Koster (SKK) internal friction peak was found to be related to atomic concentra-tion ratio, C_(La)/ C_P. La may intensify obviously the damping of SKK if C_(La)/ C_P≥2.6, and af-fect no more if C_(La)/ C_P=0.27 and P in supersatureation.
Key words:  internal friction      Snoek-Ke-Koster peak      Fe-P-La-N alloy     
Received:  18 May 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I5/21

1 戢景文,李茂华,肖连芳,高怀荪.金属学报,1981;17:293
2 戢景文,赵增祺,贺礼端,耿殿奇.物理学报,1985;34:1620
3 戢景文,魏全金、耿殿奇,吴玉琴.金属学报,1990;26:A14
4 戢景文,肖连芳、高怀荪.金属学报,1980;16:115
5 戢景文,赖祖涵,李广义,吴玉琴,张国福.金属学报,1991;27:A408
6 Nowick A S. Berry B S. Anelastic Relaxation in Crystalline Solids. New York: Academic, 1972: 263
7 Zielinski A, Lunarska E. Smialowski M. Acta Metall, 1977; 25: 551
8 1976; 42: 578
9 由淼,杨继光,陈德源.物理学报,1974;23:292
10 魏全金,戢景文,赖祖涵.待发表
11 Ino H, sugeno T. Acta Metall, 1967; 15: 1197
[1] LI Weijuan, ZHANG Hengyi, FU Hao, ZHANG Jianping, QI Xiangyu. INTERNAL FRICTION STUDY OF MECHANISM OF BAKE-HARDENING ON LOW CARBON STEEL[J]. 金属学报, 2015, 51(4): 385-392.
[2] WANG Hua SHI Wen HE Yanlin FU Renyu LI Lin. STUDY OF Mn AND P SOLUTE DISTRIBUTIONS AND THEIR EFFECT ON THE TENSILE BEHAVIOR IN ULTRA LOW CARBON BAKE HARDENING STEELS[J]. 金属学报, 2011, 47(3): 263-268.
[3] WU Jie CUI Hongzhi CHI Jing YAO Shuyu HAN Fusheng. INTERNAL FRICTION PEAK IN B2 Fe--Al ALLOYS DURING ORDERING PROCESS[J]. 金属学报, 2009, 45(4): 396-399.
[4] Jian ZHANG. EFFECTS OF GRAIN-BOUNDARY PHASES ON HYDROGEN EMBRITTLEMENT OF FE-NI-CR AUSTENITIC ALLOY BY INTERNAL FRICTION[J]. 金属学报, 2008, 44(9): 1095-1098 .
[5] SUN Wei. The internal friction peak correlated to the relaxation of Al antisite atoms in Fe-Al alloys[J]. 金属学报, 2007, 43(3): 311-314 .
[6] WANG Hongbin; WANG Xiaoyu; ZHANG Jihua; XU Zuyao T. Y. Hsu. Internal Friction of Nano--Grained Fe--25\%Ni Alloy Bulk[J]. 金属学报, 2004, 40(5): 523-526 .
[7] CHE Yunyi; LIU Fendi; ZENG Guiyi; XU Yuchang; JI Jingwen (College of Sciences; Northeastern Univerisity; Shenyang 110006)HUA Qiaozhu; LIU Jianmin; HUANG Zhenru(Institute of Iron & Steel; Baoshan Iron & Steel Company; Shanghai 201900)Correspondent: JI Jingwen; professor; Tel: (024)25915148; Fax: (024)23891072;E-mail: cos ramm. cneu. edu. cn.. Snoek-K■-kster DAMPING IN 340 MPa BAKE HARDENING STEELS[J]. 金属学报, 1998, 34(8): 831-835.
[8] WANG Weiguo; ZHOU Bangxin; ZHENG Zhongmin(Laboratory for Nuclear Fuel and Materials; Nuclear Power Institute of China; Chengdu 610041)Correspondent: WANG Weiguo; Tel: (028)5582199-88531. DAMPING CAPACITY OF Fe-Cr-Al-Si ALLOYS[J]. 金属学报, 1998, 34(10): 1039-1042.
[9] YUAN Lixi; FANG Qianfeng(Laboratory of Internal Fricion and Defects in Solids;Institute of Solid State Physics; The Chinese Academy of Sciences; Hefei 230031) Correspondents: FANG Qianfeng;professor;E-mail:qffang@issp.hfcas.ac.cn. NONLINEAR FITTING OF THE INTERNAL FRICTION DATA AND ITS APPLICATION ON THE BAMBOO GRAIN BOUNDARY RELAXATION IN PURE Al[J]. 金属学报, 1998, 34(10): 1016-1020.
[10] GE Tingsui (T S. KE); (Laboratory of Internal Friction and Defects in Solinds; Institute of Solid State Physics; Chinese Academy of Sciences; Hefei 230031). EXPERIMENTAL AND THEORETICAL STUDY ON NON-LINEAR ANELASTIC INTERNAL FRICTION[J]. 金属学报, 1997, 33(1): 9-21.
[11] LIU Junmin; ZHANG Jinxiu (Zhongshan University; Guangzhou 510275)(Manuscript received 1995-08-09; in revised form 1996-04-11). BHAVIOUR OF COMPLEX ELASTIC MODULUS AND INTERNAL FRICTION DURING EUTECTOID DECOMPOSITION[J]. 金属学报, 1996, 32(8): 785-790.
[12] LIU Junmin(Department of Physics; Zhongshan University; Guangzhou 510275);SHUI Jiapeng(Institute of Solid State Physics; Chinese Academy of Sciences; Hefei230031)(Manuscript received 1994-04-15). STRUCTURE RELAXATION OF AMORPHOUS ALLOYS[J]. 金属学报, 1995, 31(19): 318-323.
[13] JI Jingwen;SUN Yujie;LIU Yanmei(Northeastern University; Shenyang)(Manuscript received 7 September; 1993; in revised form 10 December;1993). HIGH TEMPERATURE INTERNAL FRICTION FOR Fe-Nb-C ALLOYS[J]. 金属学报, 1994, 30(5): 210-216.
[14] GUAN Xingsheng;GE Tingsui (T. S. Ke) Laboratory of Internal Friction and Defects in Solids; Institute of Solid State Physics; Academia Sinica; HefeiInstitute of Solid State Physics; Academia Sinica; Hefei 230031. INTERNAL FRICTION PEAK ASSOCIATED WITH GRAIN BOUNDARY IN Al BICRYSTALS[J]. 金属学报, 1993, 29(8): 1-4.
[15] SHUI Jiapeng; CHENG Lifang; LIU Junmin; CHU Zhaoqin (Institute of Solid State Physics; Academia Sinica; Hefei). STABILITY OF NANOCRYSTALLINE Ni-P RIBBON[J]. 金属学报, 1992, 28(9): 73-76.
No Suggested Reading articles found!