| SURFACE STATE AND CATALYTIC ACTIVITY OF ACTIVATED AMORPHOUS Fe_(80)Zr_(12)B_8 ALLOY |
| WANG Xike; SHEN Ningfu; CHEN Haisong (Zhengzhou Institute of Technology); ZHANG Haifeng(Luoyang Research Institute for Ship Materials); GU Haicheng (Xi'an Jiaotong University) |
|
Cite this article:
WANG Xike; SHEN Ningfu; CHEN Haisong (Zhengzhou Institute of Technology); ZHANG Haifeng(Luoyang Research Institute for Ship Materials); GU Haicheng (Xi'an Jiaotong University). SURFACE STATE AND CATALYTIC ACTIVITY OF ACTIVATED AMORPHOUS Fe_(80)Zr_(12)B_8 ALLOY. Acta Metall Sin, 1992, 28(8): 60-66.
|
|
|
Abstract The depth profile of composition, chemical state of elements and morphology of as-received and activated amorphous Fe_(80)Zr_(12)B_8 alloy ribbons have been studied by means of Auger electron spectroscopy, X-ray photoelectron spectroscopy and scanning Auger microprobe combined with Ar ion bombardment. Both dull and free sides of the as-received ribbons were covered with an iron oxide layer. While a pronounced surface segregation and oxidation of B were observed on both sides of activated ribbons, the fine microcrystalline α-Fe was precipitated as well as B and Zr were oxidized selectively in subsurface layer. On both sides of ribbons, a porous surface structure was formed. The BET surface area was measured to be increasing from 0.11 to 2.68 m~2/g. The principal mechanism of in situ activation has been discussed.
|
|
Received: 18 August 1992
|
1 Yokoyama A, Komiyama H, Inoue H. J Catal, 1981: 68:355 2 Yamashita H, Yoshikama M, Funabiki T, Yoshida S. J Chem Soc Faraday Trans I, 1987: 83: 2883 3 Baiker A, Schlogl R, Armbruster E, Guentherodt H-J. J Catal, 1987; 107:221 4 Kisfaludi G, Schay Z, Guczi L, Konczos G, Lovas A, Kovacsp. Appl Surf Sci,1987; 28: 111 5 Wagner C D, Riggs W M, Davis L E, Moulder J F, Muilenberg G E. In: Prairie M N ed., Handbook of X-ray Photoelectron Spectroscopy, Perkin-Elmer Co. Physical Electronics Division, 1979 6 Mavel G, Escard J, Costa P, Castaing J. Surf Sci, 1973; 35: 109 7 Walz B, Oelhafen P, Guentherodt H-J. Appl Surf Sci, 1989; 37: 337 8 Yu Xinnan, Schlapbach L. Phys Rev, 1988; 37B: 6215 9 Smithells C J. Metals Reference Book. 5th ed., London: Butterworths, 1976: 193 10 Kisfaludi G, Lazar K, Schay Z, Guzi L. Appl Surf Sci, 1985; 24: 225F |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|