| STRUCTURE AND MAGNETIC PROPERTIES OF Fe/Pd COMPOSITIONALLY MODULATED FILMS |
| ZHANG Lin; LIU Yihua(Shandong University; Jinan); WANG Hao(Dongnan University; Nanjing) |
|
Cite this article:
ZHANG Lin; LIU Yihua(Shandong University; Jinan); WANG Hao(Dongnan University; Nanjing). STRUCTURE AND MAGNETIC PROPERTIES OF Fe/Pd COMPOSITIONALLY MODULATED FILMS. Acta Metall Sin, 1992, 28(9): 77-80.
|
|
|
Abstract Fe/Pd compositionally modulated films (CMF) were prepared by vapour deposition from two sources onto glass substrate under vacuum. The modulation and crystal structures of the film were examined by X-ray diffaction. The magnetic properties were determined by vibrating sample magnetometer. The Pd layer in the Fe/Pd CMF is of fcc structure, and the Fe layer structure transits from bcc into amorphous state with decreasing thickness of Fe layer. The dependence of specific saturation magnetization on thickness of Fe layer has also been discussed.
|
|
Received: 18 September 1992
|
1 Shan Z S, Nafis S, Aylesworth K D, Sellmyer D J. J Appl Phys, 1988; 63: 3218 2 Kazama N S. In: Steeb S, Warlimont H eds., Rapidly Quenched Metals, Vol.Ⅱ, North-Holland, Amsterdam: 1985:1177 3 Hodges L, Watson R E, Ehrenreich H. Phys Rev, 1972; B5: 3953 4 李民,梅良模.物理学报,1992;待发表 5 Window B. J Appl Phys, 1988; 63: 1080 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|