STRUCTURE AND MAGNETIC PROPERTIES OF Fe/Pd COMPOSITIONALLY MODULATED FILMS
ZHANG Lin; LIU Yihua(Shandong University; Jinan); WANG Hao(Dongnan University; Nanjing)
Cite this article: 

ZHANG Lin; LIU Yihua(Shandong University; Jinan); WANG Hao(Dongnan University; Nanjing). STRUCTURE AND MAGNETIC PROPERTIES OF Fe/Pd COMPOSITIONALLY MODULATED FILMS. Acta Metall Sin, 1992, 28(9): 77-80.

Download:  PDF(327KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Fe/Pd compositionally modulated films (CMF) were prepared by vapour deposition from two sources onto glass substrate under vacuum. The modulation and crystal structures of the film were examined by X-ray diffaction. The magnetic properties were determined by vibrating sample magnetometer. The Pd layer in the Fe/Pd CMF is of fcc structure, and the Fe layer structure transits from bcc into amorphous state with decreasing thickness of Fe layer. The dependence of specific saturation magnetization on thickness of Fe layer has also been discussed.
Key words:  compositionally modulated film      modulated structure      specific saturation magnetization      Fe/Pd film     
Received:  18 September 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I9/77

1 Shan Z S, Nafis S, Aylesworth K D, Sellmyer D J. J Appl Phys, 1988; 63: 3218
2 Kazama N S. In: Steeb S, Warlimont H eds., Rapidly Quenched Metals, Vol.Ⅱ, North-Holland, Amsterdam: 1985:1177
3 Hodges L, Watson R E, Ehrenreich H. Phys Rev, 1972; B5: 3953
4 李民,梅良模.物理学报,1992;待发表
5 Window B. J Appl Phys, 1988; 63: 1080
[1] XU Zuyao (T.Y.HSU). STRENTHENING MECHANISM OF MODULATED STRUCTURE INITIATED BY SPINODAL DECOMPOSITION[J]. 金属学报, 2011, 47(1): 1-6.
[2] ZOU Zhiqiang;LI Ming;JIANG ZhihonK;LUO Caiqing; SHEN Defang (Shanghai Institute of Metallurgy; Chinese Academy of Sciences; Shanghai 200050). MAGNETIC,MAGNETO-OPTICAL PROPERTIES AND THERMAL STABILITY OF Tb/Co MULTILAYER FILMS[J]. 金属学报, 1997, 33(7): 749-755.
[3] ZHANG Liuwan; CHEN Tingguo; XIE Xiaoming; WU Xiaochu; SHITiansheng(Shanghai Institute of Metallurgy; Chinese Academy of Sciences;Shanghai 200050) LI Xiangting; GAO Jianhua; SUN Jing(Shanghai Institute of Ceramics;Chinese Academy of Sciences; Shanghai 200050). EFFECTS OF HEAT TREATMENT ON Pb-DOPED Bi-2223 SUPERCONDUCTOR[J]. 金属学报, 1995, 31(6): 277-285.
No Suggested Reading articles found!