| REACTION BETWEEN Ca_2SiO_4 AND NaFeO_2 AND OPTIMIZATION OF COMPOSITION OF SINTER IN ALUMINA PRODUCTION |
| ZHAN Qianbao;LI Ming;ZHOU Jicheng;CHEN Nianyi;QI Likuan;CHEN Jiantang Shanghai Institute of Metallurgy; Academia Sinica; Research Institute of Shandong Aluminium Factory |
|
Cite this article:
ZHAN Qianbao;LI Ming;ZHOU Jicheng;CHEN Nianyi;QI Likuan;CHEN Jiantang Shanghai Institute of Metallurgy; Academia Sinica; Research Institute of Shandong Aluminium Factory. REACTION BETWEEN Ca_2SiO_4 AND NaFeO_2 AND OPTIMIZATION OF COMPOSITION OF SINTER IN ALUMINA PRODUCTION. Acta Metall Sin, 1993, 29(2): 49-53.
|
|
|
Abstract The reaction product of Ca_2SiO_4-NaFeO_2 system has been investigated byX-ray diffraction and IR spectroscopy. The product contains CaFe_2O_4 and Na_4Ca_8(SiO_4)_5.Thermodynamical estimation also confirms that Ca_2SiO_4+NaFeO_2 is not the stable pair ofthe reciprocal salt pairs of Ca, NaSiO_4, FeO_2 system. In the reactions betweenNa_4Ca_8(SiO_4)_5 and sodium aluminate solution there forms Ca_3[Al(OH)_6]_2 (or its solid solu-tion) which will decrease the recovery of alumina. Based on the abovementioned facts, themathematical model for the optimization of the composition of sinters in alumina productionhas been explained.
|
|
Received: 18 February 1993
|
1 Chen Nianyi, Zhang Weiming, Cheng Zhaonian. In: Danzer K ed., Wissensche-ftliche Seitrage der Friedrich-Schiller Universitate, Jeaa: Friedrich-Schiller Universitate Jena, 1989: 59 2 许志宏,王乐珊.无机热化学数据库.北京:中国科学院化工冶金研究所,1981 3 戚立宽,罗玉长,杨思明.金属学报,1979;15:29 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|