| INTERNAL FRICTION PEAK ASSOCIATED WITH GRAIN BOUNDARY IN Al BICRYSTALS |
| GUAN Xingsheng;GE Tingsui (T. S. Ke) Laboratory of Internal Friction and Defects in Solids; Institute of Solid State Physics; Academia Sinica; HefeiInstitute of Solid State Physics; Academia Sinica; Hefei 230031 |
|
Cite this article:
GUAN Xingsheng;GE Tingsui (T. S. Ke) Laboratory of Internal Friction and Defects in Solids; Institute of Solid State Physics; Academia Sinica; HefeiInstitute of Solid State Physics; Academia Sinica; Hefei 230031. INTERNAL FRICTION PEAK ASSOCIATED WITH GRAIN BOUNDARY IN Al BICRYSTALS. Acta Metall Sin, 1993, 29(8): 1-4.
|
|
|
Abstract Internal friction of Al bicrystals with mis-orientation angles 60° and 129.5°was measured with forced-vibration method. Internal friction peaks vs temperature were ob-served around 200℃ (frequency 1Hz) with an activation energy of about 0.88 eV. Preliminarydiscussions were made on the mechanism of this internal friction peak.
|
|
Received: 18 August 1993
|
1 Ke T S. Phys Rev, 1947; 71: 533. 2 Ke T S, Zhang B S. phys stat sol(a), 1986; 96:515. 3 Iwasaki K. phys stat sol (a), 1985; 90:K35. 4 文亦汀,朱震刚,谢福康,杨世卿等.第二次全国固体内耗与超声衰减学术会议论文集.北京:原子能出版社,1989:125 5 Ogino Y, Amano Y. Trans Japan Inst Metals, 1979; 20: 82. 6 Kokawa H, Watanabe T, Krashima S. Phil Mag, 1981; A44: 1239. 7 Rhines F N, Bond W E, Kissel W E. Tans ASM, 1956; 48: 979. 8 Zhu A W, Ke T S. phys. stat. sol. (a), 1989; 113: 393. 9 Ke T S, Cheng B L. phys. stat. sol. (a), 1989; 115: 119. 10 Ke T S. In: Ke T S ed., Proc 9th Int Conf on Internal Friction and Ultrasonic Attenuation in Solids, Beijing: Intern. Academic Publ, Oxford: Pergamon Press, 1990: 113 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|