Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (9): 42-46    DOI:
Current Issue | Archive | Adv Search |
COMPARISON OF SOLUTE DISTRIBUTION BETWEEN SPHERICAL GROWTH AND DIRECTIONAL SOLIDIFICATION
WU Qiang;LIU Chi Nanjing University of Science and Technology Southeast University
Cite this article: 

WU Qiang;LIU Chi Nanjing University of Science and Technology Southeast University. COMPARISON OF SOLUTE DISTRIBUTION BETWEEN SPHERICAL GROWTH AND DIRECTIONAL SOLIDIFICATION. Acta Metall Sin, 1993, 29(9): 42-46.

Download:  PDF(240KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By comparing the solute distribution between spherical growth and directionalsolidification, it is found that the steady-state of solute distribution in directionalsolidification can not exist in spherical growth.
Key words:  spherical growth      solute distribution      steady-state     
Received:  18 September 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I9/42

1 《数学手册》编写组.数学手册.北京:高等教育出版社,1983:216
2 Kurz W,Fisher D J著;毛协民,包冠乾译.凝固原理.西安:西北工业大学出版社,1987:159
[1] MIN Zhixian SHEN Jun WANG Lingshui FENG Zhourong LIU Lin FU Hengzhi. MICROSTRUCTURAL EVOLUTION OF DIRECTIONALLY SOLIDIFIED Ni-BASED SUPERALLOY DZ125 UNDER PLANAR GROWTH[J]. 金属学报, 2010, 46(9): 1075-1080.
[2] CHEN Changle;LU Fuyi (Northwestern Polytechnical University; Xi'an 710072). STOCHASTIC DYNAMICS FOR NONEQUILIBRIUM SOLUTE DISTRIBUTION AT SOLID-LIQUID INTERFACE[J]. 金属学报, 1997, 33(5): 455-460.
[3] ZHANG Junshan Associate Professor;Department of Materiats Seience and Engineering;Dattan Institute of Technology;CAO Zhiben Dalian Institute of Technology. RELATIONSHIP BETWEEN CREEP BEHAVIOR AND DISLOCATION SUBSTRUCTURE IN Ni-20Cr ALLOYS[J]. 金属学报, 1988, 24(2): 111-118.
[4] LI Yanxiang;LIU Baicheng Department of Mechanical Engineering; Tsinghua University; Beijing. INITIAL COMPOSITION TRANSIENT DURING CRYSTAL GROWTH[J]. 金属学报, 1988, 24(1): 82-86.
No Suggested Reading articles found!