Acta Metall Sin  1994, Vol. 30 Issue (22): 453-458    DOI:
Current Issue | Archive | Adv Search |
IN SITU TEM OBSERVATIONS OF DISLOCATION EMISSION, MULTIPICATION AND MOTION INDUCED BY ANODIC DISSOLUTION IN TYPE 310 STAINLESS STEEL
HUANG Yizhong(Beijing Instilute of Aeronautic Materials);CHEN Qizhi(University of Science and Technology Beijing);YUAN Changyan(Beijing Institute of Aeronautic Malerials);CHU Wuyang(University of Science and Technology. Beijing)
Cite this article: 

HUANG Yizhong(Beijing Instilute of Aeronautic Materials);CHEN Qizhi(University of Science and Technology Beijing);YUAN Changyan(Beijing Institute of Aeronautic Malerials);CHU Wuyang(University of Science and Technology. Beijing). IN SITU TEM OBSERVATIONS OF DISLOCATION EMISSION, MULTIPICATION AND MOTION INDUCED BY ANODIC DISSOLUTION IN TYPE 310 STAINLESS STEEL. Acta Metall Sin, 1994, 30(22): 453-458.

Download:  PDF(379KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In situ TEM observations on the behaviour of dislocation configuration ahead of a loaded crack tip in 310 stainless steel before and after anodic dissolution were carried out in running tap water by specical constant-displacement loading stage.After eliminating the effect of creep at room temperature,the anodic dissolution may induce the dislocation emission, multiplication and motion onto 310 stainless steel in water. The SCC in water at room temperature could occur in the thin foil 310 stainless steel specimen.
Key words:  anodic dissolution      dislocation emission      in situ TEM observation     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I22/453

1RevieRW.UhligHH.ActaMetall,1974:22:6192UhligHH.JElecSci,1976:123:16693黄彦良,曹楚南.林海潮,吕明.金属学报,1993:29:B2124GuB,ChuWY,QiaoLJ.HisaoCMScrMetallMater,1994:31:1615王政富.中国科学院金属腐蚀与防护研究所博士论文,1993.6JonesDA.MetallTrans,1985:16A:11337KaufmanMJ,FinkJI.AetaMetall,1985;36:22138MagninT,ChieragattiR,OLtraR.ActaMetallMater.1990:38:13139陈奇志.褚武扬,肖纪美.中国科学,1994;24A:29110张跃,褚武扬,王燕斌.肖纪美.中国科学,1994:24A:55111HerblebG,TheilerF.WerkstKorros,1989;40:46712乔利杰.缪辉俊,褚武扬,肖纪美.中国科学,1991:21A:1218
[1] QIAN Caifu; JIANG Zhongjun; CHEN Ping; DUAN Chenghong; CUI Wenyong. Micro-Simulation of Crack Tip Plastic Zone and Dislocation-Free Zone[J]. 金属学报, 2004, 40(2): 159-162 .
[2] LI Qikai; ZHANG Yue; CHU Wuyang. MOLECULAR DYNAMICS SIMULATION OF PLASTIC DEFORMATION DURING NANOINDENTATION[J]. 金属学报, 2004, 40(12): 1238-1242 .
[3] SU Yanjing; LU Hong; WANG Yanbin; CHU Wuyang (Department of Materials Physics; University of Science and Technology Beijing; Beijing 100083). IN SITU TEM STUDY OF DISLOCATION EMISSION AND MICROCRACK NUCLEATION FOR α-Ti AFTER ADSORBING Hg[J]. 金属学报, 1998, 34(4): 337-344.
[4] HUANG Yizhong;WANG Yanbin;CHU Wugang (Department of Materials Physics; University of Science and Technology Beijing; Beijing 100083)MEI DongSheng;SU Shihuai;YU Mengwen;JI Kebing (Company of Iron and Steel of Panzhihua; Panzhihua 617067). HYDROGEN-FACILITAED DISLOCATION EMISSION,MOTION AND INITIATION OF HYDROGEN-INDUCED MICROCRACK IN RAIL STEEL[J]. 金属学报, 1998, 34(2): 134-140.
[5] LIU Xiaomin; SU Yanjing; HUANG Yizhong; CHU Wuyang(Department of Materials Physics; University of Science and Technology Beijing; Beijing 100083)Correspondent: LIU Xiaomin; Tel: (010)62332906; Fax:(010)62327283;E-mail: ljqiao@public.bta.net.cn). IN SITU TEM OBSERVATION OF EMBRITTLEMENT OF ALUMINUM ALLOY BY LIQUID METAL[J]. 金属学报, 1998, 34(10): 1021-1027.
[6] GU Biao;NIE Yifan;GAO Kewei;CHU guyana (University of Science and Technology Beijing; Beijing 100083). IN SITU TEM OBSERVATION OF HYDROGEN-INDUCED CRACKING AND STRESS CORROSION CRACKING FOR Fe_3Al[J]. 金属学报, 1997, 33(7): 709-717.
[7] SONG Renguo; ZHANG Baojin; ZENG Meiguang(Northeastern University; Shenyang 110006)(State Key Laboratory of Solidification Processing; Northwestern PolytechnicalUniversity; Xi'an 710072). THE STRESS CORROSION AND ROLE OF Mg SEGREGATED TO GRAIN BOUNDARY IN 7175 ALUMINIUM ALLOY[J]. 金属学报, 1997, 33(6): 595-601.
[8] HUANG Yizhong; CHEN Qizhi; CHU Wuyang (University of Science and Technology Beijing; Beijing 100083)(Manuscript received 1995-03-28; in revised form 1995-07-03). IN SITU TEM OBSERVATION OF SCC IN 310 STAINLESS STEEL[J]. 金属学报, 1996, 32(1): 39-45.
[9] GU Biao; ZHANG Jingwu; WAN Farong; CHU Wuyang(Deportment of Materials Physics; University of Sci ence and Tech nology; Beijing; Beijing 100083). IN SITU TEM OBSERVATION OF DISLOCATION EMISSION, MOTION INDUCED BY ANODIC DISSOLUTION AND THE INITIATION OF SCC IN BRASS THIN FOIL[J]. 金属学报, 1995, 31(4): 156-164.
[10] GAO Kewei;CHU Wuyang;XIAO Jimei(University of Science and Technology Beijing;Beijing 100083)(Manuscript received 1995-02-27). IN SITU TEM OBSERVATION OF DISLOCATION EMISSION,MOTION AND SCC INITIATION IN Ti_3Al+Nb UNDER METHANOL CORROSION[J]. 金属学报, 1995, 31(23): 477-483.
[11] WEI Xuejun;LI Jin;ZHOU Xiangyang;KE Wei(Corrosion Scicnce Laboratory; Institute of Corrosion and Protection of Metals; Chinese Academy of Scicnces;Shenyang). SURFACE AND BULK DEFORMATION NEAR CRACK TIP FOR PURE COPPER UNDER APPLIED ANODIC CURRENT[J]. 金属学报, 1994, 30(21): 393-397.
[12] CAO Chunan;LIN Haichao;LU Ming Corrosion Science Laborotory; Institute of Corrosion and Protection of Metals; Academia Sinica; ShenyangHUANG Yanliang;Ph D student;Institute of Corrosion and Protection of Metals ;Aeudemia Sinica;Shenyang 110015. SCC MECHANISM OF AISI 321 IN ACIDIC CHLORIDE SOLUTION[J]. 金属学报, 1993, 29(5): 68-73.
[13] WANG Zhengfu;ZHU Ziyong;KE Wei;ZHANG Yun;HU Zhuangqi Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang; Institue of Metal Research; Academia Sinica; Shenyang. STRESS CORROSION PERFORMANCE OF Al-Li-Cu-Mg ALLOY[J]. 金属学报, 1992, 28(4): 58-62.
[14] LU Ke;WANG Jingtang National Laboratory for RSA; Institute of Metal Research; Academia Sinica. Shenyang; DONG Lin Liaoning Provincial Centre of Analysis and Testing Research. Shenyang. IN SITU OBSERVATION ON DYNAMIC CRYSTALLIZATION IN AMORPHOUS Ni-P ALLOY FOIL[J]. 金属学报, 1991, 27(1): 108-114.
[15] FANG Zhaoheng;CHEN Jiayong Institute of Chemical Metallurgy; Academia Sinica; Beijing. ELECTROCHEMICAL STUDIES ON ANODIC DISSOLUTION OF SYNTHETIC NICKEL SULPHIDES[J]. 金属学报, 1988, 24(6): 463-470.
No Suggested Reading articles found!