Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (6): 241-247    DOI:
Current Issue | Archive | Adv Search |
MORPHOLOGY AND HIGH RESOLUTION IMAGE OF EUTECTOID TRANSFORMATION PRODUCTS OF Ti-H ALLOYS
KANG Qiang;ZHANG Caibei;LAI Zuhan;NING Xiaoguang(Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Department of Materials Science; College of Science; Northeastern University;Shenyang 110006)
Cite this article: 

KANG Qiang;ZHANG Caibei;LAI Zuhan;NING Xiaoguang(Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Department of Materials Science; College of Science; Northeastern University;Shenyang 110006). MORPHOLOGY AND HIGH RESOLUTION IMAGE OF EUTECTOID TRANSFORMATION PRODUCTS OF Ti-H ALLOYS. Acta Metall Sin, 1995, 31(6): 241-247.

Download:  PDF(596KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The morphology and the fine structure of the hydrides in Ti-H alloys, containing 0.2-1.53 wt-% hydrogen, were investigated by TEM. It was found that the eutectoid transformation products from β-Ti(H) were consisted of δ hydrides and α-Ti,forming a micro-polycrystalline aggregate, while γ hydride was precipitated from α-Ti(H) directly. The atomic structure of these microcrystals were carefully delineated by HRTEM, showing that there may be ten variants of α-Ti around δ hydrides, which can keep two definite crystallographic relationships with α-Ti. The shear mechanism of the eutectoid transformation is discussed.
Key words:  Ti-H alloy      δ hydride      HRTEM      eutectoid transformation     
Received:  18 June 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I6/241

1NumakuraH,KoiwaM.ActaMetall,1984;32(10):17992NumakuraH,KoiwaM,AsanoH,IzumiF.ActaMetall,1988;36(8):22673BourretA,LasalmonieA,NakaS.ScrMetall,1986;20:8614KasukabeY,YamadaY,BursillLA.PhilosMag,1993;A67(1):735ZhangCB,KangQ,LaiZH.ActaMetallMater,1994;42(7):25556XiaoHZ.ScrMetallMater,1992;27:5717张彩碚,赖祖涵,计蓉,于瀛大.材料科学进展,1993;7(6):4618LenningGA,CraigheadCM,JaffeeRI.TransMetallSocAIME,1954;200:3679BurgersWG.Physica,1933—1934;I:561
[1] LI Xiaolin, WANG Zhaodong. INTERPHASE PRECIPITATION BEHAVIORS OF NANOMETER-SIZED CARBIDES IN A Nb-Ti-BEARING LOW-CARBON MICROALLOYED STEEL[J]. 金属学报, 2015, 51(4): 417-424.
[2] YU Ximo, ZHAO Shijin. STUDY ON Cu PRECIPITATE OF THE LOW C HIGH STRENGTH STEEL CONTAINING Cu AND Ni DURING ISOCHRONAL TEMPERING[J]. 金属学报, 2013, 49(5): 569-575.
[3] XU Gang CHU Dafeng CAI Linling ZHOU Bangxin WANG Wei PENG Jianchao. INVESTIGATION ON THE PRECIPITATION AND STRUCTURAL EVOLUTION OF Cu-RICH NANOPHASE IN RPV MODEL STEEL[J]. 金属学报, 2011, 47(7): 905-911.
[4] LI Longfei LI Wei SUN Zuqing YANG Wangyue. MICROSTRUCTURE REFINEMENT OF EUTECTOID STEEL BASED ON DIVORCED EUTECTOID TRANSFORMATION[J]. 金属学报, 2009, 45(6): 704-710.
[5] Rong Wang. A HRTEM study on a modulation structure in NiAl3 after ion etching[J]. 金属学报, 2008, 44(10): 1153-1156 .
[6] MAO Jian.fu;HE Liantong;YE Hengqiang(Laboratory of Atomic Imaging of Solids;Ihstitute of Metal Research;Chinese Academy of Sciences;Shenyang 110015) YANG Dezhuang;TANG Zhixiu(Harbin Institute of Technotogy;Harbin 150001)(Manuscript received 1994-07-05;in revised form 1995-02-24). HRTEM STUDY ON CRYSTAL STRUCTURE OF Zr_4Co_4Si_7 COMPOUND[J]. 金属学报, 1995, 31(7): 289-293.
No Suggested Reading articles found!