PREPARATION OF NANOMETER POWDER BY ELECTROHYDRODYNAMIC TECHNIQUE
YU Xifeng; CHENG Lizhi; HU Huosheng; LIU Xiang; HU Zhuangqi (State Key Laboratory for RSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)( Northeastern University; Shenyang 110006)(Manuscript received 1995-04-12; in revised form 1995-09-11)
Cite this article:
YU Xifeng; CHENG Lizhi; HU Huosheng; LIU Xiang; HU Zhuangqi (State Key Laboratory for RSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)( Northeastern University; Shenyang 110006)(Manuscript received 1995-04-12; in revised form 1995-09-11). PREPARATION OF NANOMETER POWDER BY ELECTROHYDRODYNAMIC TECHNIQUE. Acta Metall Sin, 1996, 32(1): 75-79.
Abstract The Sn-Bi nanometer powder was prepared by the electrohydrodynamic technique with quartz capillary nozzle. The processing parameters have been investigated.With the increase in DC voltage and the decrease in diameter of capillary nozzle, the particulate size of the Sn-Bi nanometer powder will be reduced. Moreover, the pressure feeding into the molten alloy is also an important factor controlling particulate size.Correspondent YU Xifeng,(Department of Materials Science, Northeastern University, Shenyang 110006)
DAI Changhong; ZHANG Xianpeng(Notheastern University;Shenyang 110006);ZHANG Jinsong; YANG Youjin; CAO Lihua; XIA Fei(Institute of Metal Research;Chinese Academy of Sciences; Shenyang 110015). SYNTHESIS OF NANOMETER ALUMINIUM NITRIDE POWDER BY MICROWAVE METHOD[J]. 金属学报, 1996, 32(11): 1221-1226.
[2]
LIU Xiang; ZOU Li; HU Huosheng; ZHANG Guozhi; CHENG Lizhi (Northeastern University; Shenyang); HU Zhuangqi (State Key Laboratory of RSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang)(Manuscript received 4 April; 1994). MICROSTRUCTURE OF Sn-Bi NANOMETER POWDER PREPARED BY ELECTROHYDRODYNAMIC TECHNIQUE[J]. 金属学报, 1994, 30(23): 499-502.