WANG Zhenjun; CHANG Xiangrong; PING Jueyun; TIAN Zhongzhuo; XIAO Jimei (University of Science and Technology Beijing; Beijing 100083); WEN Lishi (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-03-03; in revised form 1995-07-21 ). STRUCTURE AND MAGNETISM OF DC-MAGNETRON SPUTTERING Fe / Ti PERIODICAL NANO-MULTILAYERS. Acta Metall Sin, 1996, 32(1): 85-90.
|
Abstract A series of Fe/Ti periodical nano-miltilayers was prepared by DC-magnetron sputtering. The modulation period is between 2.2 and 24 nm. The structure of the specimens was examined by TEM and small-or high-angle X-ray diffraction technique. Their magnetism was also studied by the vibratory sample magnetometer and Mossbauer spectrum. The face-centred cubic Fe was found in multilayers containing thinner Fe layers nearby 2 nm. The saturation magnetization increases and the coercivity decreases with increasing modulation period.Correspondent: WANG Zhenjun,(Department of Materials Physics, University of Science and Technology Beijing, Beijing 100083)
|
Received: 18 January 1996
|
1RenardJP.JMaterSciTechnol.1993:9:12DoyamaM,MatsuiM,MatsuokaH,MatsuokaS,MitaniS,DoiK.JMagnMagnMater,1991:93:3743PanF,YangT,ZhangJ,LiuBX.JPhysCondensMatter,1993;5:L5074LeDangK,VeilletP,BeauvillainP,ChappertC,HeHui,LamelasFJ,LeeCH,ClarkeRoy.PhysRev.1991;B43:132285YamamotoB.SurTechnol(Japanese),1988;40:10586BaloghJ,RodmacyB,ChanberodA.SolidStateComm.1988;66(2):1437RodmacgB,HillairetJ,LaugierJ,ChanberodA.JPhysCondensMatter,1990;2:958BaiHY,CheeH,ZhangY,WangWK.PhysStatSolid.1993;125:1259GuYS,ChaiWP,MaiZH,ZhouJG,MeiLM,DongC,FeeW,ChenH.PhysRew.1994;B50:611 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|