Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (1): 85-90    DOI:
Current Issue | Archive | Adv Search |
STRUCTURE AND MAGNETISM OF DC-MAGNETRON SPUTTERING Fe / Ti PERIODICAL NANO-MULTILAYERS
WANG Zhenjun; CHANG Xiangrong; PING Jueyun; TIAN Zhongzhuo; XIAO Jimei (University of Science and Technology Beijing; Beijing 100083); WEN Lishi (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-03-03; in revised form 1995-07-21 )
Cite this article: 

WANG Zhenjun; CHANG Xiangrong; PING Jueyun; TIAN Zhongzhuo; XIAO Jimei (University of Science and Technology Beijing; Beijing 100083); WEN Lishi (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-03-03; in revised form 1995-07-21 ). STRUCTURE AND MAGNETISM OF DC-MAGNETRON SPUTTERING Fe / Ti PERIODICAL NANO-MULTILAYERS. Acta Metall Sin, 1996, 32(1): 85-90.

Download:  PDF(336KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A series of Fe/Ti periodical nano-miltilayers was prepared by DC-magnetron sputtering. The modulation period is between 2.2 and 24 nm. The structure of the specimens was examined by TEM and small-or high-angle X-ray diffraction technique. Their magnetism was also studied by the vibratory sample magnetometer and Mossbauer spectrum. The face-centred cubic Fe was found in multilayers containing thinner Fe layers nearby 2 nm. The saturation magnetization increases and the coercivity decreases with increasing modulation period.Correspondent: WANG Zhenjun,(Department of Materials Physics, University of Science and Technology Beijing, Beijing 100083)
Key words:  Fe / Ti multilayer      γ-Fe      DC-magnetron sputtering     
Received:  18 January 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I1/85

1RenardJP.JMaterSciTechnol.1993:9:12DoyamaM,MatsuiM,MatsuokaH,MatsuokaS,MitaniS,DoiK.JMagnMagnMater,1991:93:3743PanF,YangT,ZhangJ,LiuBX.JPhysCondensMatter,1993;5:L5074LeDangK,VeilletP,BeauvillainP,ChappertC,HeHui,LamelasFJ,LeeCH,ClarkeRoy.PhysRev.1991;B43:132285YamamotoB.SurTechnol(Japanese),1988;40:10586BaloghJ,RodmacyB,ChanberodA.SolidStateComm.1988;66(2):1437RodmacgB,HillairetJ,LaugierJ,ChanberodA.JPhysCondensMatter,1990;2:958BaiHY,CheeH,ZhangY,WangWK.PhysStatSolid.1993;125:1259GuYS,ChaiWP,MaiZH,ZhouJG,MeiLM,DongC,FeeW,ChenH.PhysRew.1994;B50:611
No related articles found!